Std ID |
Description (Standard Title) |
|
GB/T 36791-2018
|
Determination of bromine in organic flame retardant -- Oxygen bomb combustion-ion selective electrode method
|
|
GB/T 36793-2018
|
Determination of plasticizers in rubber-plastics -- Gas chromatography-mass spectrometry method
|
|
GB/T 36804-2018
|
Liquid silicone rubber -- Classification and system nomenclature
|
|
GB/T 7755.1-2018
|
Rubber, vulcanized or thermoplastic -- Determination of permeability to gases -- Part 1: Differential-pressure methods
|
|
GB/T 1232.4-2017
|
Rubber, unvulcanized -- Determinations using a shearing-disc viscometer -- Part 4: Determination of the Mooney stress-relaxation rate
|
|
GB/T 15906-2017
|
Determination of isobutylene-isoprene rubber or polyisobutylene content in rubber
|
|
GB/T 18866-2017
|
Rubber -- Dissolution by acid digestion
|
|
GB/T 6031-2017
|
Rubber, vulcanized or thermoplastic -- Determination of hardness (hardness between 10 IRHD and 100 IRHD)
|
|
GB/T 7764-2017
|
Rubber identification -- Infrared spectrometric method
|
|
GB/T 34692-2017
|
Thermoplastic elastomer -- Determination of halogen -- Oxygen bomb combustion-ion chromatography
|
|
GB/T 34715-2017
|
Thermoplastic elastomer -- Determination of phthalates -- Gas chromatography-mass spectrometry
|
|
GB/T 4498.2-2017
|
Rubber -- Determination of ash -- Part 2: Thermogravimetric analysis
|
|
GB/T 24131.2-2017
|
Rubber, raw -- Determination of volatile-matter content -- Part 2: Thermogravimetric methods using an automatic analyser with an infrared drying unit
|
|
GB/T 35492-2017
|
Determination of organotin content of latex products -- GC-MS method
|
|
GB/T 33324-2016
|
Determination of heavy metal content of latex products -- Inductively coupled plasma atomic emission spectrometry
|
|
GB/T 1232.1-2016
|
Rubber, unvulcanized -- Determinations using a shearing-disc viscometer -- Part 1: Determination of Mooney viscosity
|
|
GB/T 1687.1-2016
|
Rubber, vulcanized -- Determination of temperature rise and resistance to fatigue in flexo meter testing -- Part 1: Basic principles
|
|
GB/T 1687.3-2016
|
Rubber, vulcanized -- Determination of temperature rise and resistance to fatigue in flexo meter testing -- Part 3: Compression flexo meter (constant-strain type)
|
|
GB/T 33046-2016
|
Rubber products -- Determination the content of cobalt -- Atomic absorption spectrometry
|
|
GB/T 33078-2016
|
Rubber -- Identification of anti-degradants -- Gas chromatography/mass spectrometry
|
|
GB/T 33095.1-2016
|
Rubber, unvulcanized -- Measurement of rheological properties using rotorless shear rheometer -- Part 1: Frequency sweep
|
|
GB/T 33402-2016
|
Silicone rubber compound -- General purpose
|
|
GB/T 33422-2016
|
Thermoplastic elastomer -- Determination of heavy metal contents -- Inductively coupled plasma atomic emission spectrometric method
|
|
GB/T 33429-2016
|
Silicone rubber compounds -- High tear strength type and high tensile strength type
|
|
GB/T 33430-2016
|
Silicone rubber compounds -- Application for wires and cables
|
|
GB/T 4499-2016
|
Rubber, vulcanized -- Determination of anti-degradants -- Thin layer chromatographic method
|
|
GB/T 6029-2016
|
Rubber, vulcanized -- Determination of accelerants -- Thin layer chromatographic method
|
|
GB/T 20726-2015
|
Microbeam analysis -- Selected instrumental performance parameters for the specification and checking of energy dispersive X-ray spectrometers for use in electron probe microanalysis
|
|
GB/T 13642-2015
|
Rubber, vulcanized or thermoplastic -- Resistance to ozone cracking -- Dynamic strain testing
|
|
GB/T 15255-2015
|
Rubber, vulcanized -- Test method for artificial weathering -- Carbon-arc lamp
|
|
GB/T 32365-2015
|
Silicone rubber compound -- Classification and system nomenclature
|
|
GB/T 7759.1-2015
|
Rubber, vulcanized or thermoplastic -- Determination of compression set -- Part 1: At ambient or elevated temperatures
|
|
GB/T 15252-2014
|
Plastics and ebonite - Determination of indentation hardness by means of a durometer (shore hardness)
|
|
GB/T 3512-2014
|
Rubber, vulcanized or thermoplastic -- Accelerated ageing and heat resistance tests -- Air-oven method
|
|
GB/T 7762-2014
|
Rubber, vulcanized or thermoplastic -- Resistance to ozone cracking -- Static strain test
|
|
GB/T 13936-2014
|
Rubber, vulcanized -- Method for determination of strength properties of adhesive to metal in shear by tension loading
|
|
GB/T 13939-2014
|
Rubber, vulcanized -- Test method of heat and oxygen -- Tube tester ageing method
|
|
GB/T 14837.1-2014
|
Rubber and rubber products -- Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -- Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers
|
|
GB/T 14837.2-2014
|
Rubber and rubber products -- Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -- Part 2: Acrylonitrile-butadiene and halobutyl rubber
|
|
GB/T 15254-2014
|
Rubber, vulcanized -- Determination of adhesion to metal-180 Degree Peel test method
|
|
GB/T 15256-2014
|
Rubber or thermoplastic rubber, vulcanized -- Determination of low-temperature brittleness (multiple test piece method)
|
|
GB/T 16586-2014
|
Rubber, vulcanized -- Determination of adhesion to wire cord
|
|
GB/T 1689-2014
|
Rubber vulcanized -- Determination of abrasion resistance (Akron machine)
|
|
GB/T 29613.2-2014
|
Rubber -- Analysis by pyrolytic gas-chromatographic methods -- Part 2: Determination of styrene/butadiene/isoprene ratio
|
|
GB/T 31063-2014
|
Extractables in aqueous autoclavates for pharmaceutical closures of butyl rubber
|
|
GB/T 31357-2014
|
Compounded rubber -- General technical specification
|
|
GB/T 3517-2014
|
Rubber, raw natural -- Determination of plasticity retention index (PRI)
|
|
GB/T 7759.2-2014
|
Rubber, Vulcanized or thermoplastic -- Determination of compression set at low temperatures
|
|
GB/T 9869-2014
|
Rubber -- Measurement of vulcanization characteristics with the oscillating disc curemeter
|
|
GB/T 11210-2014
|
Rubber, vulcanized or thermoplastic -- Antistatic and conductive products -- Determination of electrical resistance
|
|
GB/T 13646-2013
|
Rubber -- Determination of bound styrene content -- Spectrophotometric method
|
|
GB/T 29607-2013
|
Rubber product -- Determination of cadmium content -- Atomic absorption spectrometry
|
|
GB/T 29608-2013
|
Rubber product -- Determination of phthalate acid esters
|
|
GB/T 29609-2013
|
Rubber -- Determination of phenol and biphenyl-A
|
|
GB/T 29610-2013
|
Rubber products -- Determination of polybrominated biphenyls and polybrominated diphenyl ethers -- Gas chromatography and mass spectrometry
|
|
GB/T 29611-2013
|
Rubber, raw -- Determination of the glass transition temperature -- Differential scanning calorimetry (DSC)
|
|
GB/T 29613.1-2013
|
Rubber -- Analysis by pyrolytic gas-chromatographic methods -- Part 1: Identification of polymers (single polymers and polymer blends)
|
|
GB/T 29614-2013
|
Determination the content of polycyclic aromatic hydrocarbons in vulcanized rubber compounds
|
|
GB/T 29616-2013
|
Thermoplastic elastomer -- Determination of polycyclic aromatic hydrocarbons -- Gas chromatography-mass spectrometry
|
|
GB/T 29644-2013
|
Rubber, vulcanized -- Determination the content of N-phenyl-β-naphthylamine -- High performance liquid chromatographic method
|
|
GB/T 10541-2013
|
Rubber hose, oil suction and discharge, offshore mooring
|
|
GB/T 4497.2-2013
|
Rubber -- Determination of total sulfur content -- Part 2: Sodium peroxide fusion method
|
|
GB/T 4498.1-2013
|
Rubber -- Determination of ash -- Part 1: Muffle furnace method
|
|
GB/T 28607-2012
|
Determination of compatibility between standard elastomeric materials and automotive engine oil
|
|
GB/T 28728-2012
|
Determination of the microstructure of solution-polymerized SBR
|
|
GB/T 14833-2011
|
Synthetic materials track surfaces
|
|
GB/T 7528-2011
|
Rubber and plastics hoses and hose assemblies -- Vocabulary
|
|
GB/T 1690-2010
|
Rubber, vulcanized or thermoplastic -- Determination of the effect of liquids
|
|
GB/T 25262-2010
|
Rubber, vulcanized or thermoplastic -- Abrasion testing -- Guidance
|
|
GB/T 25268-2010
|
Rubber -- Guide to the use of curemeter
|
|
GB/T 25269-2010
|
Rubber -- Guide to the calibration of test equipment
|
|
GB/T 25270-2010
|
Rubber and plastics test equipment -- Tensile, flexural and compression types (constant rate of traverse) -- Specification
|
|
GB/T 4497.1-2010
|
Rubber -- Determination of total sulfur content -- Part 1: Oxygen combustion flask method
|
|
GB/T 24153-2009
|
Rubber and Elastomer Materials - Determination of N-nitrosaminess
|
|
GB/T 528-2009
|
Rubber, vulcanized or thermoplastic -- Determination of tensile stress-strain properties
|
|
GB/T 14834-2009
|
Rubber, vulcanized or thermoplastic -- Determination of tendency to adhere to and corrode metals
|
|
GB/T 14838-2009
|
Rubber and rubber products -- Determination of precision for test method standards
|
|
GB/T 1681-2009
|
Rubber -- Determination of rebound resilience of vulcanizates
|
|
GB/T 23651-2009
|
Rubber, vulcanized or thermoplastic -- Hardness testing -- Introduction and guide
|
|
GB/T 23655-2009
|
Test for the cure level of compound latex
|
|
GB/T 24130-2009
|
Flexible Packaging latex sampling
|
|
GB/T 24131-2009
|
Determination of volatile raw rubber content
|
|
GB/T 24143-2009
|
Rubber and rubber products -- Determination of the sensitivity of test methods
|
|
GB/T 2942-2009
|
Rubber, vulcanized -- Determination of static adhesion to textile cord -- H-pull test
|
|
GB/T 531.2-2009
|
Rubber, vulcanized or thermoplastic -- Determination of indentation hardness -- Part 2: IRHD pocket meter method
|
|
GB/T 7757-2009
|
Rubber, vulcanized or thermoplastic -- Determination of compression stress-strain properties
|
|
GB/T 11205-2009
|
Determination of thermal conductivity of rubber wire method
|
|
GB/T 11206-2009
|
Standard test method for rubber deterioration -- Surface cracking
|
|
GB/T 529-2008
|
Rubber, vulcanized or thermoplastic -- Determination of tear strength (Trouser, angle and crescent test pieces)
|
|
GB/T 1233-2008
|
Rubber, unvulcanized -- Determinations of pre-vulcanization characteristic using a shearing disc viscometer
|
|
GB/T 12830-2008
|
Rubber, vulcanized or thermoplastic -- Determination of shear modulus and adhesion to rigid plates -- Quadruple shear methods
|
|
GB/T 12832-2008
|
Rubber -- Determination of crystallization effects by hardness measurements
|
|
GB/T 13248-2008
|
Rubber and rubber latices -- Determination of manganese content -- Sodium periodate photometric methods
|
|
GB/T 15251-2008
|
Rubber -- Determination of free sulfur
|
|
GB/T 15340-2008
|
Rubber, raw natural and raw synthetic -- Sampling and further preparative procedures
|
|
GB/T 16583-2008
|
Identification of saturated rubbers in unsaturated rubbers
|
|
GB/T 1685-2008
|
Rubber, vulcanized or thermoplastic -- Determination of stress relaxation in compression at ambient and at elevated temperatures
|
|
GB/T 1688-2008
|
Rubber, vulcanized -- Determination of tension fatigue
|
|
GB/T 1692-2008
|
Vulcanized rubber - Determination of the insulation resistivity
|
|
GB/T 3511-2008
|
Rubber, vulcanized or thermoplastic -- Resistance to weathering
|