US$169.00 · In stock Delivery: <= 3 days. True-PDF full-copy in English will be manually translated and delivered via email. GB/T 25414-2010: Thickness limit and test method of mulch film for cotton planting Status: Valid
| Standard ID | Contents [version] | USD | STEP2 | [PDF] delivered in | Standard Title (Description) | Status | PDF |
| GB/T 25414-2010 | English | 169 |
Add to Cart
|
3 days [Need to translate]
|
Thickness limit and test method of mulch film for cotton planting
| Valid |
GB/T 25414-2010
|
PDF similar to GB/T 25414-2010
Basic data | Standard ID | GB/T 25414-2010 (GB/T25414-2010) | | Description (Translated English) | Thickness limit and test method of mulch film for cotton planting | | Sector / Industry | National Standard (Recommended) | | Classification of Chinese Standard | G33 | | Classification of International Standard | 83.140.10 | | Word Count Estimation | 7,724 | | Date of Issue | 2010-11-10 | | Date of Implementation | 2011-03-01 | | Regulation (derived from) | National Standard Approval Announcement 2010 No.8 (Total No.163) | | Issuing agency(ies) | General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, Standardization Administration of the People's Republic of China | | Summary | This standard specifies the cotton planting mulch thickness limits and determination. This standard applies to cotton planting mulch. |
GB/T 25414-2010: Thickness limit and test method of mulch film for cotton planting---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order.
Tickness limit and test method of mulch film for cotton planting
ICS 83.140.10
G33
National Standards of People's Republic of China
Cotton planting and Determination of film thickness limits
Issued on. 2010-11-10
2011-03-01 implementation
Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China
Standardization Administration of China released
Foreword
The standard proposed by China Machinery Industry Federation.
This standard by the National Standardization Technical Committee (SAC/TC201) Agricultural machinery centralized.
This standard was drafted. Xinjiang agricultural Machinery Testing Station, Xinjiang agricultural machinery pipe
Authority.
The main drafters of this standard. Eagle Zhang, Xu Min, Gao Yan, Pei Xinmin.
Cotton planting and Determination of film thickness limits
1 Scope
This standard specifies the limits for cotton planting and film thickness measurement method.
This standard applies to cotton planting mulch.
2 Film thickness limits
Cotton planting film thickness limit of not less than 0.008mm.
3 Determination
3.1 measuring instrument
3.1.1 thickness gauge with a resolution of 1μm.
3.1.2 The meter should have a planar surface and a lower surface measuring surface flat or convex surface on the measurement, all measuring surface should be
Polished surface.
3.1.3 the vertical measuring surface is a plane/plane, each measuring surface diameter should be 2.5mm ~ 10mm between two parallel plane is not less than
5μm, measured surface should be adjusted to meet the above requirements. Measurement should face between the load applied to the specimen in 0.5N ~ 1.0N.
3.1.4 When the vertical measuring surface is convex/plane, the radius of curvature measurement should be between 15mm ~ 50mm in diameter should be measured at the surface
Not less than 5mm, the face should be measured between the load applied to the specimen in 0.1N ~ 0.5N.
3.1.5 transfer output measured values \u200b\u200bcan use mechanical method (micrometer), an optical method (using a mirror meter) or electrical method (inductive method)
A variety of methods.
3.2 Preparation of the sample
Away from the longitudinal ends of the sample at about 1m, transversely across the width of the test specimens, specimen width 100mm. Except for the submission of folding or packing
Stack samples, specimens should be free of wrinkles, nor should other defects.
3.3 Determination of step
3.3.1 sample at (23 ± 2) ℃ condition conditioning at least 1h, a thin film of humidity, conditioning time and the environment should be the test material
Norms or negotiated by the supply and demand sides.
3.3.2 The measurement should be checked before each measurement sample surface and measuring instrument should be no oil, dust and other contamination.
3.3.3 should be checked before measuring gauge zero. After each set of sample measurements should re-examine its zero point.
3.3.4 should be measured down gently probe to avoid deformation of the specimen.
3.3.5 equidistant length measuring method to determine the position of the point of thickness, as follows.
a) the sample length is less than equal to 300mm, measuring 10 points;
b) in the sample length between 300mm ~ 1500mm, measuring 20 points;
c) the sample length is greater than equal to 1500mm, measured at least 30 points.
The samples did not cut edges should start measuring 50mm away from the edges.
3.4 Data Processing
Measuring the sample thickness is the arithmetic mean of all the measurements.
Tips & Frequently Asked Questions:Question 1: How long will the true-PDF of GB/T 25414-2010_English be delivered?Answer: Upon your order, we will start to translate GB/T 25414-2010_English as soon as possible, and keep you informed of the progress. The lead time is typically 1 ~ 3 working days. The lengthier the document the longer the lead time. Question 2: Can I share the purchased PDF of GB/T 25414-2010_English with my colleagues?Answer: Yes. The purchased PDF of GB/T 25414-2010_English will be deemed to be sold to your employer/organization who actually pays for it, including your colleagues and your employer's intranet. Question 3: Does the price include tax/VAT?Answer: Yes. Our tax invoice, downloaded/delivered in 9 seconds, includes all tax/VAT and complies with 100+ countries' tax regulations (tax exempted in 100+ countries) -- See Avoidance of Double Taxation Agreements (DTAs): List of DTAs signed between Singapore and 100+ countriesQuestion 4: Do you accept my currency other than USD?Answer: Yes. If you need your currency to be printed on the invoice, please write an email to [email protected]. In 2 working-hours, we will create a special link for you to pay in any currencies. Otherwise, follow the normal steps: Add to Cart -- Checkout -- Select your currency to pay.
|