Chinese Standards Shop Partner of Google-Books Database: 169759 (Nov 10, 2019)
 HOME   Quotation   Tax   Examples Standard-List   Contact-Us   View-Cart
  

SY/T 6151-2009

Chinese Standard: 'SY/T 6151-2009'
Standard IDContents [version]USDSTEP2[PDF] delivered inStandard Title (Description)StatusRelated Standard
SY/T 6151-2009English140 Add to Cart 0--15 minutes. Auto immediate delivery. Assessment of corroded steel pipelines Valid SY/T 6151-2009
SY/T 6151-2009Chinese14 Add to Cart <=1-day [PDF from Chinese Authority, or Standard Committee, or Publishing House]

 SY/T 6151-2009 -- Click to view a PDF In 0~10 minutes time, full copy of this English-PDF will be auto-immediately delivered to your email by our cloud-server.  
Detail Information of SY/T 6151-2009; SY/T6151-2009
Description (Translated English): Assessment of corroded steel pipelines
Sector / Industry: Oil & Gas Industry Standard (Recommended)
Classification of Chinese Standard: E10
Classification of International Standard: 75.010
Word Count Estimation: 11,117
Date of Issue: 2009-12-01
Date of Implementation: 2010-05-01
Older Standard (superseded by this standard): SY/T 6151-1995
Quoted Standard: GB/T 228; GB/T 21143; SY/T 6597
Drafting Organization: China National Petroleum Corporation Pipeline Company (including the original Northeast oil Authority)
Administrative Organization: Oil and Gas Storage and Transportation Standardization Technical Committee
Regulation (derived from): National Energy Board Notice 2009 No. 2; industry standard filing Notice 2010 No. 2 (No. 122 overall)
Summary: This standard specifies the in-service pipelines containing corrosion damage evaluation method. This standard applies to blunt, low stress concentration corrosion damage of carbon and low alloy steel pipes evaluation. Blunt pipeline mechanical damage assessment could refer to this standard.

SY/T 6151-2009
    Page 1 of 14
SY
PETROLEUM AND NATURAL GAS INDUSTRY STANDARD
OF THE PEOPLE’S REPUBLIC OF CHINA
ICS 75-010
E 10
Registration number. 27482-2010
Replacing SY/T 6151-1995
Assessment of corroded steel pipelines
钢质管道管体腐蚀损伤评价方法
ISSUED ON. DECEMBER 01, 2009
IMPLEMENTED ON. MAY 01, 2010
Issued by. National Energy Administration
    Page 2 of 14
Table of contents
Foreword ... 3 
1 Scope ... 4 
2 Normative references ... 4 
3 Requirements for assessment personnel ... 4 
4 Raw data preparation before assessment ... 5 
5 Corrosion area measurement ... 5 
5.1 Measurement method ... 5 
5.2 Corrosion-pit depth measurement ... 5 
5.3 Longitudinal length measurement ... 5 
5.4 Circumferential length measurement ... 5 
6 Pipe corrosion damage assessment category-classification ... 6 
7 Pipe corrosion damage size assessment method ... 6 
7.1 Assessment based on corrosion-pit’s relative depth ... 6 
7.2 Assessment based on corrosion-pit’s longitudinal length ... 7 
7.3 Effect of circumferential corrosion scale ... 7 
8 Maximum safe operating pressure assessment method ... 8 
8.1 Maximum safe operating pressure calculation ... 9 
8.2 Assessment of corrosion damage category ... 9 
8.3 Overall assessment process ... 10 
Appendix A ... 11 
Appendix B ... 14 
    Page 3 of 14
Foreword
Pipeline corrosion damage causes the pipe body to form various shape and
size defects. Serious defects can lead to pressure pipeline leak or rupture
accident, which impacts the safe and smooth operation of pipeline. Therefore,
as for the damaged pipeline, proposing a scientific assessment method has
become a pressing need for the pipeline industry.
This Standard replaces SY/T 6151-1995 “Assessment of corroded steel
pipelines”.
Compared with SY/T 6151-1995, the main changes are as follows.
- MODIFY the corrosion damage assessment category content (Chapter 6 of
this edition);
- USE Rstreng’s yield strength calculation equation to replace the yield
strength calculation equation under ASME B31G-1991 which is referenced
in SY/T 6151-1995 (Clause 8.1 of this edition);
- MODIFY the assessment threshold of corrosion damage category (Clause 8.2
of this edition).
The Appendix A and B of this Standard are normative.
This Standard was proposed by and shall be under the jurisdiction of Gas
Storage and Transportation Standardization Technical Committee.
The drafting organizations of this Standard. China National Petroleum Pipeline
Company Limited (including the original Northeast Oil Transportation Authority),
Chinese Academy of Sciences Institute of Metal Research.
Main drafters of this Standard. Chen Jianfeng, Han Enhou, Zhang Huabing,
Feng Qingshan, Yu Jingchun, Li Shaozhong, Zhang Bo, Ke Wei, Wang Xueli,
Song Hancheng, Wang Fuxiang.
This Standard replaces the previous standard as follows.
- SY/T 6151-1995.
    Page 4 of 14
Assessment of corroded steel pipelines
1 Scope
This Standard specifies the method for assessment of corrosion damage of in
service pipeline.
This Standard applies to the assessment of blunt, low stress concentration
corrosion damage carbon steel and low alloy steel pipeline. The assessment of
pipeline’s blunt mechanical damage can be conducted in accordance with this
Standard.
This Standard does not apply to the assessment of the steel pipeline which is
before installation or in installation process, or the assessment of the steel
pipelines which have serious defects in weld and heat affected zone.
This Standard applies only to the internal pressure bearing pipeline; when the
pipeline is withstanding a big additional stress, it shall be considered separately.
2 Normative references
The provisions in following documents become the provisions of this Standard
through reference in this Standard. For dated references, the subsequent
amendments (excluding corrigendum) or revisions do not apply to this Standard,
however, parties who reach an agreement based on this Standard are
encouraged to study if the latest versions of these documents are applicable.
For undated references, the latest edition of the referenced document applies.
GB/T 228 Metallic materials - Tensile testing at ambient temperature
GB/T 21143 Metallic materials - Unified method of test for determination of
quasi-static fracture toughness
SY/T 6597 Technical standard of intelligent pigging on steel pipeline
3 Requirements for assessment personnel
Assessment personnel shall have the following basic knowledge and abilities.
a) Pipeline work principles and safe operation precautions.
    Page 5 of 14
b) Basic knowledge on material corrosion and mechanical properties.
c) Identification and measurement of field corrosion state.
4 Raw data preparation before assessment
Raw data shall include the following.
a) Pipeline diameter, wall thickness, material, mechanical properties AND
manufacturers.
b) Transmission medium, working pressure, temperature, AND the latest
pressure test conditions.
c) Corrosion environment and corrosion protection conditions.
d) Pipeline operating history, such as pipe age, leak history, AND larger
maintenance and repair works, etc.
5 Corrosion area measurement
5.1 Measurement method
5.1.1 As for corrosion defects, the intelligent internal detection can be used,
which is detailed in SY/T 6597.
5.1.2 As for corrosion defects, it is also allowed to use the external detection
method such as calipers, straight ruler, tape measure, ultrasonic thickness
gauge AND other measuri......
Related standard:   SY/T 6150.1-2017  SY/T 6156-2017
   
 
Privacy   ···   Product Quality   ···   About Us   ···   Refund Policy   ···   Fair Trading   ···   Quick Response
Field Test Asia Limited | Taxed in Singapore: 201302277C | Copyright 2012-2019