US$154.00 · In stock Delivery: <= 3 days. True-PDF full-copy in English will be manually translated and delivered via email. GB/T 7690.6-2013: Reinforcements -- Test method for yarns -- Part 6: Determination of twist balance index Status: Valid GB/T 7690.6: Evolution and historical versions
Standard ID | Contents [version] | USD | STEP2 | [PDF] delivered in | Standard Title (Description) | Status | PDF |
GB/T 7690.6-2013 | English | 154 |
Add to Cart
|
3 days [Need to translate]
|
Reinforcements -- Test method for yarns -- Part 6: Determination of twist balance index
| Valid |
GB/T 7690.6-2013
|
GB/T 7690.6-2001 | English | 199 |
Add to Cart
|
2 days [Need to translate]
|
Reinforcements -- Test method for yarns -- Part 6: Determination of twist balance index
| Obsolete |
GB/T 7690.6-2001
|
GB/T 7690.6-1989 | English | RFQ |
ASK
|
3 days [Need to translate]
|
Textile glass--Yarns--Determination of twist balance index
| Obsolete |
GB/T 7690.6-1989
|
PDF similar to GB/T 7690.6-2013
Basic data Standard ID | GB/T 7690.6-2013 (GB/T7690.6-2013) | Description (Translated English) | Reinforcements -- Test method for yarns -- Part 6: Determination of twist balance index | Sector / Industry | National Standard (Recommended) | Classification of Chinese Standard | Q36 | Classification of International Standard | 59.100.10 | Word Count Estimation | 8,841 | Older Standard (superseded by this standard) | GB/T 7690.6-2001 | Quoted Standard | ISO 291 | Adopted Standard | ISO 3343-2010, IDT | Regulation (derived from) | National Standards Bulletin No. 18 of 2013 | Issuing agency(ies) | General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, Standardization Administration of the People's Republic of China | Summary | This standard specifies the method for the determination of glass fiber, carbon fiber, aramid fiber or other reinforcing fibers and cables made of plied yarn twist balance index. |
GB/T 7690.6-2013: Reinforcements -- Test method for yarns -- Part 6: Determination of twist balance index ---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order.
.. Reinforcements Test method for yarns Part 6. Determination of twist balance index
ICS 59.100.10
Q36
National Standards of People's Republic of China
Replacing GB/T 7690.6-2001
Test method for yarns reinforced
Determination of twist balance index. Part 6
Part 6. Determinationoftwistbalanceindex
(ISO 3343.2010, Reinforcementyarns-
Determinationoftwistbalanceindex, IDT)
Issued on. 2013-09-18
2014-06-01 implementation
Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China
Standardization Administration of China released
Foreword
GB/T 7690 "Test method for yarns enhanced" is divided into six sections.
--- Part 1. Determination of linear density;
--- Part 2. Determination of twist;
--- Part 3. Glass fiber breaking force and elongation measurement;
--- Part 4. Determination of stiffness;
--- Part 5. Determination of glass fiber diameter of the fiber;
--- Part 6. Determination of twist balance index.
This section GB/T Section 67690 of.
This section drafted in accordance with GB/T 1.1-2009 given rules.
This Part replaces GB/T 7690.6-2001 "enhanced method for yarns - Part 6. Determination of twist balance index", and
GB/T 7690.6-2001 compared to, in addition to editorial changes outside the main technical changes are as follows.
--- In a broader range of applications, in addition to the original standard glass fiber coated carbon fiber and aramid fiber yarn, but also includes other
Reinforcing fibers (see Chapter 1);
--- Remove the "Reference Standards" GB/T 18374, an increase of ISO 291 (see Chapter 2, Section 2 of the 2001 edition);
--- Remove the "Definitions" chapter (see Chapter 3 of the 2001 edition);
--- Added "sample" and "test the humidity and the environment" chapters (see Chapter 4, Chapter 5).
This section uses the translation method identical with ISO 3343.2010 "Enhanced yarn twist balance index determination", made the following editorial
modify.
--- Modify the standard name.
The correspondence between the consistency of the international normative documents referenced in our country with the following documents.
--- GB/T 2918-1998 plastic sample conditioning and testing of the standard environment (ISO 291.1997, IDT).
This part of the National Standardization Technical Committee fiberglass (SAC/TC245) centralized.
This section is responsible for drafting. Nanjing Fiberglass Research and Design Institute Limited, the national glass fiber product quality supervision and inspection center.
The main drafters of this section. Xu Qi, Wang Yumei, Huang Ying, Chen Shang, Shi Zhuo, Fang Yunwei.
This standard replaces the standards previously issued as follows.
--- GB/T 7690.6-1989, GB/T 7690.6-2001.
Test method for yarns reinforced
Determination of twist balance index. Part 6
1 Scope
GB/T 7690 provisions of this part of the ply yarns and cables made of glass fiber, carbon fiber, aramid fiber or other reinforcing fibers
Determination of twist balance index.
2 Normative references
The following documents for the application of this document is essential. For dated references, only the dated version suitable for use herein
Member. For undated references, the latest edition (including any amendments) applies to this document.
ISO 291 environmental standard plastic sample conditioning and testing (Plastics-Standardatmospherefor
conditioningandtesting)
Principle 3
The yarn is put into a predetermined length and width of the opening of the coil, and count the number of twist yarns own making.
4 Sample
A unit of product 1) or laboratory sample 2) continuous take five samples were measured.
5 conditioning and testing environment
Without the humidity. In case of disputes, the temperature should be specified in ISO 291 is (23 ± 2) ℃, relative humidity of (50 ± 10)% of the standard environment
Under conditions.
6 Operating
6.1 start package tangential direction to return 50m yarns to obtain a representative sample. With the thumb and forefinger of yarn, but not
Take it off.
6.2 tangentially drawn 1m yarn as a sample, according to the 6.1, with the other hand and hold the other end of the sample, but do not cut off. The sample was vacant
And forming an opening at both ends of the coil of 100mm apart.
6.3 Record opening coils twist self-inflicted (Ni) and twist the coil (S or Z). You can use the untwisting of the twist count method
Slither.
1) per unit of product. the smallest unit of a commercially available usual delivery of products.
2) laboratory samples is part of the unit of the product, the product is not easy when the unit into the laboratory, take a laboratory sample, from which the desired and cut samples.
|