YS/T 775.1-2011: Methods for chemical analysis of lead anode slime. Part 1: Determination of lead content. Na2EDTA titrimetric method
Status: Valid
Standard IDUSDBUY PDFLead-DaysStandard Title (Description)Status
YS/T 775.1-2011159 Add to Cart 3 days Methods for chemical analysis of lead anode slime. Part 1: Determination of lead content. Na2EDTA titrimetric method Valid

Similar standards

GB/T 3884.2   GB/T 3884.1   YS/T 710.6   YS/T 775.3   YS/T 775.4   YS/T 775.2   

Basic data

Standard ID: YS/T 775.1-2011 (YS/T775.1-2011)
Description (Translated English): Methods for chemical analysis of lead anode slime. Part 1: Determination of lead content. Na2EDTA titrimetric method
Sector / Industry: Nonferrous Metallurgy Industry Standard (Recommended)
Classification of Chinese Standard: H13
Classification of International Standard: 77.120.01
Word Count Estimation: 6,638
Date of Issue: 2011-12-20
Date of Implementation: 2012-07-01
Regulation (derived from): ?MIIT Announcement 2011 No.43
Issuing agency(ies): Ministry of Industry and Information Technology
Summary: This standard specifies the determination of lead anode mud lead content. This standard applies to the determination of lead anode mud lead content. Measuring range: 5. 00% to 15. 00%.

YS/T 775.1-2011: Methods for chemical analysis of lead anode slime. Part 1: Determination of lead content. Na2EDTA titrimetric method


---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order.
Methods for chemical analysis of lead anode slime.Part 1. Determination of lead content.Na2EDTA titrimetric method ICS 77.120.01 H13 People's Republic of China Nonferrous Metals Industry Standard Methods for chemical analysis of lead anodes Part 1. determination of lead content Na2EDTA titration Part 1. Determination ofleadcontent- 2011-12-20 release 2012-07-01 Implementation Issued by the Ministry of Industry and Information Technology of the People's Republic of China

Foreword

YS/T 775-2011 "lead anode mud chemical analysis method" is divided into seven parts. - Part 1. Determination of lead content - Na2EDTA titration; Part 2. Determination of Bismuth Flame Atomic Absorption Spectrometry and Na2EDTA Titration; - Part 3. Determination of arsenic content - Potassium bromate titration; - Part 4. Determination of antimony content - Flame atomic absorption spectrometry and cerium sulphate titration; - Part 5. Determination of gold and silver; - Part 6. Determination of copper content - Iodometric method; Part 7. Determination of arsenic, copper and selenium - Inductively coupled plasma atomic emission spectrometric method. This section is part 1. This part is drafted in accordance with the rules given in GB/T 1.1-2009. This part is the national nonferrous Metals Standardization Technical Committee (SAC/TC243). This part is responsible for drafting units. Shaanxi Dongling Smelting Co., Ltd. This part participates in the drafting unit. Beijing Mining and Metallurgy Research Institute, China Metallurgical Huludao Nonferrous Metals Group Corporation, Zhuzhou Smelting Group Co., Ltd. Company, Henan Yuguang Gold Lead Co., Ltd. The main drafters of this part are. Zhou Wei, Che Hongfang, Meng Lijuan, Liu Chunfeng, Tang Shufang, Yu Li, Chi Fenghua, Li Zunyi, Guo Jun, Huang Xiaogang, Yang Linjuan. Methods for chemical analysis of lead anodes Part 1. determination of lead content Na2EDTA titration

1 Scope

This part of YS/T 775 specifies the determination of lead in lead anodic mud. This part is applicable to the determination of lead in lead anodic mud. The measurement range is 5.00% ~ 15.00%.

2 method summary

Samples with nitric acid, hydrochloric acid dissolved in sulfuric acid medium, with hydrobromic acid to eliminate arsenic, antimony and tin interference, lead lead sulfate precipitation and coexistence Elemental separation, in pH 5.5 acetic acid - sodium acetate buffer solution, the precipitation into lead acetate, thiourea masking a small amount of copper, ascorbic acid masking A small amount of iron interference to xylenol orange as an indicator, with Na2EDTA standard titration solution titration from purple to bright yellow as the end.

3 reagent

Unless otherwise stated, only the reagents identified as analytical reagents and distilled or deionized water or comparable purity were used in the analysis. 3.1 ascorbic acid. 3.2 Hydrochloric acid (ρ1.19g/mL). 3.3 nitric acid (ρ1.42g/mL). 3.4 Sulfuric acid (ρ1.84g/mL). 3.5 hydrobromic acid (ρ 1.38 g/mL). 3.6 Thiourea (saturated solution). 3.7 Sulfuric acid (5 95). 3.8 xylenol orange solution (5g/L). 3.9 tartaric acid solution (100g/L). 3.10 acetic acid - sodium acetate buffer solution (pH5.5). Weigh 375g of anhydrous sodium acetate, add water, add 50mL glacial acetic acid, water Diluted to.2000mL, mix well. 3.11 Na2EDTA standard titration solution (0.02 mol/L). 3.11.1 Preparation. Weigh 7.4g ethylenediamine tetraacetic acid disodium in a 300mL beaker, add water to slightly heat dissolve, cool to room temperature, move in 1000mL volumetric flask, diluted with water to the mark, mix, place after 3 days calibration. 3.11.2 Calibration. Weigh four 0.1500g metal lead (w (Pb) ≥99.99%), accurate to 0.0001g, placed in 300mL beaker , Add 10mL nitric acid (3.3) heated to completely dissolved, remove the slightly cold, add 10mL sulfuric acid (3.4), heated to smoke, remove the cooling, The following is done in accordance with 5.4.2. Calculate the amount of Na2EDTA standard titration solution according to formula (1) Concentration. c = m0 (V1-V0) · M × 1000 (1) Where. c - Na2EDTA standard titration solution of the amount of material concentration, the unit is mol per liter (mol/L);
......
Image     

Tips & Frequently Asked Questions:

Question 1: How long will the true-PDF of YS/T 775.1-2011_English be delivered?

Answer: Upon your order, we will start to translate YS/T 775.1-2011_English as soon as possible, and keep you informed of the progress. The lead time is typically 1 ~ 3 working days. The lengthier the document the longer the lead time.

Question 2: Can I share the purchased PDF of YS/T 775.1-2011_English with my colleagues?

Answer: Yes. The purchased PDF of YS/T 775.1-2011_English will be deemed to be sold to your employer/organization who actually pays for it, including your colleagues and your employer's intranet.

Question 3: Does the price include tax/VAT?

Answer: Yes. Our tax invoice, downloaded/delivered in 9 seconds, includes all tax/VAT and complies with 100+ countries' tax regulations (tax exempted in 100+ countries) -- See Avoidance of Double Taxation Agreements (DTAs): List of DTAs signed between Singapore and 100+ countries

Question 4: Do you accept my currency other than USD?

Answer: Yes. If you need your currency to be printed on the invoice, please write an email to Sales@ChineseStandard.net. In 2 working-hours, we will create a special link for you to pay in any currencies. Otherwise, follow the normal steps: Add to Cart -- Checkout -- Select your currency to pay.