HOME   Cart(0)   Quotation   About-Us Tax PDFs Standard-List Powered by Google www.ChineseStandard.net Database: 189759 (1 Dec 2024)

GB/T 12914-2018 Related PDF English (GB/T 12914-2008, GB/T 12914-1991)

GB/T 12914-2018 (GB/T12914-2018, GBT 12914-2018, GBT12914-2018) & related versions
Standard IDContents [version]USDSTEP2[PDF] delivered inStandard Title (Description)See DetailStatusSimilar PDF
GB/T 12914-2018English170 Add to Cart 0-9 seconds. Auto delivery. Paper and board -- Determination of tensile properties -- Constant rate of elongation method (20mm/min) GB/T 12914-2018 Valid GBT 12914-2018
GB/T 12914-2008English140 Add to Cart 0-9 seconds. Auto delivery. Paper and board -- Determination of tensile properties GB/T 12914-2008 Obsolete GBT 12914-2008
GB/T 12914-1991English279 Add to Cart 3 days Paper and board--Determination of tensile properties--Constant rate of elongation method GB/T 12914-1991 Obsolete GBT 12914-1991
Buy with any currencies (Euro, JPY, KRW...): GB/T 12914-2018    Preview this PDF: GB/T 12914-2018



GB/T 12914-2018 NATIONAL STANDARD OF THE PEOPLE’S REPUBLIC OF CHINA ICS 85.010 Y 30 Replacing GB/T 12914-2008 Paper and Board - Determination of Tensile Properties - Constant Rate of Elongation Method (20 mm/min) [ISO 1924-2:2008, Paper and Board - Determination of Tensile Properties - Part 2: Constant Rate of Elongation Method (20 mm/min), MOD] ISSUED ON: DECEMBER 28, 2018 IMPLEMENTED ON: JULY 1, 2019 Issued by: State Administration for Market Regulation; Standardization Administration of the People’s Republic of China. Table of Contents Foreword ... 3  1 Scope ... 6  2 Normative References ... 6  3 Terms and Definitions ... 7  4 Principle ... 8  5 Instruments ... 8  6 Adjustment and Calibration of Tester ... 10  7 Sample Preparation and Processing ... 10  8 Test Procedures ... 11  9 Calculation and Result Report ... 12  10 Precision ... 15  11 Test Report ... 16  Appendix A (normative) Calibration of Tensile Tester ... 18  Appendix B (informative) A Comparison of Symbols between this Standard and ISO 1924-2:2008 ... 19  Foreword This Standard was drafted in accordance with the rules in GB/T 1.1-2009. This Standard serves as a replacement of GB/T 12914-2008 Paper and Board - Determination of Tensile Properties. In comparison with GB/T 12914-2008, the main technical changes are as follows: ---The title of the Standard is modified; ---The Scope is modified (see Chapter 1; Chapter 1 of Version 2008); ---A statement of differences between this Standard of GB/T 22898-2008 [ISO 1924-3:2005, MOD] is added (see NOTE of Chapter 1); ---The terms and definitions are modified (see Chapter 3): the definitions of elongation (see 3.3) and strain (see 3.4) are added; ---Relevant content of constant-rate loading method is deleted (see Chapter 4 of Version 2008); standard chapters are re-arranged; ---Strain measurement accuracy is modified into elongation measurement accuracy (see 5.1; 5.2.1.1 of Version 2008); supplementary statement of elongation measurement accuracy is added (see Note 2 of 5.1); ---The calculation formula of breaking length is added (see 9.5); ---The calculation formula of modulus of elasticity is modified (see 9.8; 10.8 of Version 2008); ---Relevant data of precision is added (see Table 2 and Table 3 of 10.3). This Standard adopts the re-drafting method to modify and adopt ISO 1924-2:2008 Paper and Board - Determination of Tensile Properties - Part 2: Constant Rate of Elongation Method (20 mm/min). In comparison with ISO 1924-2:2008, the main technical differences and their causes are as follows: ---In terms of Normative References, this Standard adjusts the technical differences, so as to adapt to the technical conditions in China. The adjustments are intensively reflected in Chapter 2 “Normative References”. See the specific adjustments below:  GB/T 450, which modifies and adopts international standard, is used to replace ISO 186; Paper and Board - Determination of Tensile Properties - Constant Rate of Elongation Method (20 mm/min) 1 Scope This Standard stipulates the method of using test instrument with a constant rate of elongation (20 mm/min) to determine tensile strength, strain at break, breaking length and tensile energy absorption of paper and board. It also stipulates the calculation formulas of tensile index, tensile energy absorption and index and modulus of elasticity. This Standard is applicable to all papers and boards, except corrugated paperboards. NOTE: GB/T 22898-2008 Paper and Board - Determination of Tensile Properties - Constant Rate of Elongation Method (100 mm/min) (ISO 1924-3:2005, MOD) stipulates another form of constant rate elongation method: using 100 mm/min constant rate of elongation and 100 mm test length. For different samples, the rate of elongation has different effects on tensile strength, strain at break, tensile energy absorption and modulus of elasticity. Under most circumstances, when the rate of elongation increases from 20 mm/min (180 mm test length) to 100 mm/min (100 test length), tensile strength increases 5% ~ 15%. The test results obtained through the two methods should not be compared with each other. 2 Normative References The following documents are indispensable to the application of this document. In terms of references with a specified date, only versions with a specified date are applicable to this document. In terms of references without a specified date, the latest version (including all the modifications) is applicable to this document. GB/T 450 Paper and Board - Sampling for Testing and Identification of Machine and Cross Direction, Wire Side and Felt Side (GB/T 450-2008, ISO 186:2002, MOD) GB/T 451.2 Paper and Board - Determination of Grammage (GB/T 451.2-2002, eqv ISO 536:1995) GB/T 451.3 Paper and Board - Determination of Thickness (GB/T 451.3-2002, idt ISO 534:1988) GB/T 10739 Paper, Board and Pulps - Standard Atmosphere for Conditioning and Testing (GB/T 10739-2002, eqv ISO 187:1990) 3.9 Modulus of Elasticity Modulus of elasticity refers to the maximum slope of the tensile force - elongation curve multiplied by the initial test length, and then, divided by the product of the width and thickness of the sample. NOTE: refer to Figure 2. 4 Principle Use a tensile tester, at a constant rate of elongation, stretch a sample of the specified size to break; record its tensile force. If necessary, record its elongation. If the tensile force and elongation can be continuously recorded, then, strain at break, tensile energy absorption and modulus of elasticity can be determined. Through the recorded data and known quantification of samples, tensile index and tensile energy absorption index can be calculated. 5 Instruments 5.1 Tensile Tester 5.1.1 Tensile tester shall be able to stretch a sample of the specified size at a constant rate of elongation (20 mm/min), determine its tensile force, and if necessary, determine its elongation. 5.1.2 The maximum allowable error of the tensile tester’s tensile force determination and display device is ± 1%. If necessary, the maximum allowable error of its elongation determination and display device is ± 0.1%. Tensile force may be recorded as a function of elongation on electronic integrator or other equivalent devices. NOTE 1: the measurement accuracy of elongation is of great importance. In order to accurately determine the actual elongation, it is recommended to install an appropriate extensometer directly on the sample, so as to avoid false elongation of the sample due to the imperceptible slippage of the sample in the chuck and the tightening of the connecting part of the instrument. The latter depends on the applied load. In terms of instruments that have been used for a period of time, due to the wear of the connecting parts, the error will increase. The additional load caused by the installation of the extensometer on the sample should be controlled within the required allowable error limit of tensile force. NOTE 2: if the determination result of elongation is merely used for the calculation of strain at break and tensile energy absorption, then, the elongation determination accuracy of ± 0.1 mm is acceptable. 5.1.3 Tensile tester includes two chucks, which are used to clamp samples of the energy absorption needs to be determined, this device shall be used. NOTE: some tensile testers are equipped with the function of calculating tensile energy absorption without external connection with the above-mentioned devices. 5.4 Device for Drawing a Tensile Force - Elongation Curve and Measuring the Maximum Slope of the Curve It is only needed when the modulus of elasticity needs to be determined. NOTE: some tensile testers are equipped with the function of drawing the tensile force- elongation curve and calculating the modulus of elasticity without external connection with the above-mentioned devices. 6 Adjustment and Calibration of Tester 6.1 Install the instrument in accordance with the instruction manual. If necessary, in accordance with Appendix A, calibrate the tensile force determination device and elongation determination device of the instrument. 6.2 Adjust the position of the chucks, so that the test length (the distance between the two clamping lines) is (180 ± 1) mm. NOTE: under certain circumstances, for example, high-strain papers or length-limited samples, a smaller test length may be used. Under this circumstance, it is recommended to adjust the rate of elongation to (10 ± 2.5) % of the initial test length; indicate the adopted test length and rate of elongation in the rest report. 6.3 In the chuck, clamp a thin aluminum foil; measure the distance between the two clamping indentations; check whether the test length is accurate. 6.4 Adjust the chuck separation rate (sample elongation rate) to (20 ± 5) mm/min. 6.5 Adjust the clamping pressure, so that the sample has no slippage or damage. NOTE: in terms of some papers and paperboards, the sample might quickly break (within 5 s) or take a long time (for example, more than 30 s) to break. Under this circumstance, different rates of elongation may be used; indicate the rates of elongation in the test report. 7 Sample Preparation and Processing 7.1 Sampling In accordance with GB/T 450, take samples. 7.2 Temperature and Humidity Treatment In accordance with the stipulations of GB/T 10739, conduct temperature and humidity treatment on the sample. In addition, under such atmospheric conditions, prepare samples for the tests. 7.3 Sample Preparation 7.3.1 From non-damaged paper and paperboard samples, cut sample strips with a width of (15 ± 0.1) mm and a length sufficient to be clamped between two chucks. Avoid using bare hands to touch the part of the sample between the two chucks. The test area must be free of watermarks, creases and wrinkles. If watermark must be included, it shall be indicated in the test report. The two long sides of the sample shall be flat and straight. Within the entire clamping length, the parallelism error shall not exceed ± 0.1 mm. The incision of the sample shall be neat and damage-free. Cut a sufficient number of sample strips, so as to ensure that there are 10 valid determination results in each direction (longitudinal or transverse). NOTE: some papers are difficult to be evenly cut, two or three layers of paper may be sandwiched in a harder paper (for example, bond paper) to form a stack, then cut the samples. 7.3.2 If tensile index or tensile energy absorption index needs to be determined, then, in accordance with the stipulations of GB/T 451.2, determine the quantification of the samples. 7.3.3 If the modulus of elasticity needs to be determined, then, in accordance with the stipulations of GB/T 451.3, determine the sample thickness. 8 Test Procedures 8.1 Check the zero position of the tester and the recorder (if necessary). 8.2 Adjust the chuck distance to the specified initial test length; clamp the sample on the chucks. Pay attention not to use your hands to touch the test area between the two clamping lines. It is recommended to wear disposable gloves or lightweight cotton gloves when handling the samples. Straighten and firmly clamp the sample without leaving any perceptible loosening or obvious strain. Make sure that the sample is parallel to the direction of the applied tension (see Figure 1). NOTE 1: when the instrument clamps the sample in the vertical direction, in order to prevent the sample from loosening, a small weight may be attached to the lower end of the sample, for example, a 10 g weight may be attached to a low- quantitative paper. This method is not suitable for high-strain papers. NOTE 2: for certain types of paper, it is difficult to distinguish “perceptible loosening” Appendix A (normative) Calibration of Tensile Tester In accordance with the frequency of use, regularly calibrate the instrument. It is recommended to calibrate at least once a month. Use a weight with already-known mass and a maximum allowable error of ± 0.1% to calibrate the instrument’s force-measuring device and recording device (if necessary). In accordance with the mass of the weight and the acceleration of gravity, calculate the applied force. In addition, calibration devices, for example, a pre-calibrated elastic calibration body, may also be used. Under the loaded state, within the required elongation measurement range, use a Vernier caliper or block gauge to calibrate the elongation-measuring device and recording device (if necessary) of the tensile tester. Some tensile testers’ tensile force measuring devices may stretch after being stressed. At different points within the effective operating range of the instrument, simultaneously calibrate the tensile force and elongation measuring device, so as to ensure that the measurement results are not affected. If the integrator is used to measure and determine tensile energy absorption, then, within the corresponding measuring range of tensile force and elongation, in accordance with the instruction manual, calibrate the integrator. Check whether the chucks comply with the requirements of 5.1.3 and 5.1.4. Check the drawing device used for the determination of the modulus of elasticity. ......


GB/T 12914-2008 GB NATIONAL STANDARD OF THE PEOPLE’S REPUBLIC OF CHINA ICS 85-010 Y 30 Replacing GB/T 453-2002, GB/T 12914-1991 Paper and Board – Determination of Tensile Properties (ISO 1924-1.1992, Paper and Board – Determination of Tensile Properties – Part 1. Constant Rate of Loading Method, ISO 1924-2.1994, Paper and Board – Determination of Tensile Properties – Part 2. Constant Rate of Elongation Method, MOD) ISSUED ON. AUGUST 19, 2008 IMPLEMENTED ON. MAY 1, 2009 Issued by. General Administration of Quality Supervision, Inspection and Quarantine; Standardization Administration of PRC. Table of Contents Forward ... 3  1 Scope ... 5  2 Normative References ... 5  3 Terms and Definitions ... 5  4 Method A – Constant Rate of Loading Method ... 6  5 Method B – Constant Rate of Elongation Method ... 8  6 Sampling ... 9  7 Temperature & Humidity Treatment ... 9  8 Preparation of Specimen ... 9  9 Test Steps ... 10  10 Calculation of Results ... 12  11 Accuracy ... 15  12 Test Report ... 16  Appendix A ... 17  Appendix B ... 18  Appendix C ... 19  Forward The constant rate of loading method in this Standard modifies-adopts ISO 1924-1.1992 Paper and Board – Determination of Tensile Properties – Part 1. Constant Rate of Loading Method; while constant rate of elongation method is consistent with ISO 1924-2.1994 Paper and Board – Determination of Tensile Properties – Part 2. Constant Rate of Elongation Method. This Standard’s differences with ISO 1924-1.1922 are shown in Appendix C. This Standard is the combination of GB/T 453-2002 Paper and Board – Determination of Tensile Properties – Constant Rate of Loading Method AND GB/T 12914-1991. Paper and Board – Determination of Tensile Properties – Constant Rate of Elongation Method. This Standard replaces GB/T 453-2002 and GB/T 12914-1991 at the same time. Compared with GB/T 453-2002 and GB/T 12914-1991, this Standard has the following changes. -- Normative references GB/T 451.2-2002 and QB/T 3704-1999 are added; -- Reduce the width error of specimen; -- Add the definition of modulus of elasticity. This Standard’s Appendix A is normative, while Appendix B and Appendix C are informative. This Standard was proposed by China Light Industry Council. This Standard shall be under the jurisdiction of China Standardization Technical Committee of Papermaking Industry. Drafting organization of this Standard. China National Pulp and Paper Research Institute. Chief drafting staff of this Standard. Shi Ji. The previous versions and publication of the standards replaced by this Standard include. -- GB/T 453-1989, GB/T 453-2002; -- GB/T 12914-1991. This Standard shall be interpreted by China Standardization Technical Committee of Paper and Board – Determination of Tensile Properties 1 Scope This Standard specifies two methods to determine the tensile strength of paper and board. constant rate of loading method, and constant rate of elongation method. This Standard is applicable to all papers and boards except corrugated board. 2 Normative References The provisions in following documents become the provisions of this Standard through reference in this Standard. For dated references, the subsequent amendments (excluding corrigendum) or revisions do not apply to this Standard; however, parties who reach an agreement based on this Standard are encouraged to study if the latest versions of these documents are applicable. For undated references, the latest edition of the referenced document applies. GB/T 450 Paper and Board - Sampling for Testing and Identification of Machine and Cross direction, Wire Side and Felt Side (GB/T 450-2000, ISO 186.2002, MOD) GB/T 451.2 Paper and Board - Determination of Grammage (GB/T 451.2-2002, eqv ISO 536.1995) GB/T 451.3 Paper and board - Determination of thickness (GB/T 451.3-2002, idt ISO534.1998) GB/T 10739 Paper, Board and Pulps - Standard Atmosphere for Conditioning and Testing (GB/T 10739-2002, eqv ISO 187-1990) 3 Terms and Definitions The following terms and conditions are applicable to this Standard. 3.1 Tensile strength Under condition specified in standard test method, the maximum tension that the Note 2). Note 1. If the existing commercial tester is not improved, then it is impossible for all paper type test to reach such rate (in order to accelerate the routine test, the breaking time of 10s±5s shall be taken, but the obtained result is 2% larger than the specified method result). Note 2. In order to meet the requirement that the change of loading rate does not exceed 5%, the pendulum bob instrument shall not be operated at the swing angle of more than 50°. Tensile strength tester shall contain the components mentioned in Clause 4.2.1.1 and Clause 4.2.1.2. 4.2.1.1 Accuracy of tensile strength tester shall be ±1%. Note. Although many constant rate of loading instruments are used to determine the elongation rate, the measurement accuracy is very low. Thus, such method is not recommend to determine the elongation rate; when the latter is needed to be determined, the constant rate of stretching instrument with electronic amplification and records function is recommended to use. 4.2.1.2 Clamping chuck. two, in order to grip the specimen (see Chapter 8) with specified width, each clamping chuck shall grip the specimen along the full width in one line, while the specimen shall not be damaged or slid. The clamping chuck shall be equipped with the component to adjust the clamping force. The clamping surfaces of clamping chuck shall be in the same plane, and the specimen during the test process shall also be in the above plane. Note. Clamping chuck grips the specimen between cylindrical surface and the plane, or between two cylindrical surfaces, the specimen surface shall be tangent to the cylindrical surface. If the specimen is not damaged or slid during the test process, then other types of clamping chucks can also be used. In the loading process, the parallelism between the clamping lines shall be maintained within 1°, and the clamping line shall keep vertical with force direction and specimen side length at the deviation no less than 1° (see Figure 1). The distance between clamping lines shall be adjusted to the specified test length, and the deviation shall not exceed ±1mm. elongation rate accurately, proper recording instrument is recommended to be placed on the specimen, in this case, it can avoid obvious elongation during the testing process. For instance, specimen occurs imperceptible relaxation on the clamping chuck, or the specimen relaxes due to the slide of instrument connector. The latter is caused by the wearing of the instrument; meanwhile it is related to the applied load. 5.2.1.2 Clamping chuck. see Clause 4.2.1.2. 5.2.2 Cutting device. cut the specimen to the specified dimension. 5.2.3 Online tester. if it is integrator, the reading accuracy shall be ±1%. During the testing process, the different lengths of specimens can be analyzed automatically. If the tensile energy absorption needs to be measured, then such instrument can be used. 5.2.4 Draw the curve of tensile stress – elongation rate, and determine the maximum slope device of such curve; if modulus of elasticity needs to be measured, then such instrument can be used. 6 Sampling Conduct sampling as per GB/T 450. 7 Temperature & Humidity Treatment Specimen shall be conducted temperature & humidity treatment as per GB/T 10739; prepare the specimen under the same atmospheric condition, and then test it. 8 Preparation of Specimen 8.1 If breaking length, tensile index and tensile energy absorption index are needed, then the quantitative shall be measured as per GB/T 451.2. 8.2 If modulus of elasticity is needed, then the thickness shall be measured as per GB/T 451.3. Note. If the accurate value of modulus of elasticity is needed to obtain, then the thickness of each specimen shall be measured separately rather than measuring the average thickness of specimen as per the provision of GB/T 451.3. However, the anvil diameter of thickness gauge specified in GB/T 451.3 shall be 16mm, thus, as for the specimen with width of 15mm, its suffering pressure may be slightly larger than the specified 100kPa. Therefore, the modulus of elasticity measured in this method is only an estimated value. Adjust the load of clamping chuck, so that to guarantee that the specimen has no slide or damage during the testing pro... ......

BASIC DATA
Standard ID GB/T 12914-2018 (GB/T12914-2018)
Description (Translated English) Paper and board -- Determination of tensile properties -- Constant rate of elongation method (20mm/min)
Sector / Industry National Standard (Recommended)
Classification of Chinese Standard Y30
Classification of International Standard 85.010
Word Count Estimation 12,179
Date of Issue 2018-12-28
Date of Implementation 2019-07-01
Older Standard (superseded by this standard) GB/T 12914-2008
Quoted Standard GB/T 450; GB/T 451.2; GB/T 451.3; GB/T 10739
Adopted Standard ISO 1924-2-2008, MOD
Drafting Organization Sichuan Changjiang Papermaking Instrument Co., Ltd.
Administrative Organization National Paper Industry Standardization Technical Committee
Regulation (derived from) National Standard Announcement No. 17 of 2018
Proposing organization China Light Industry Federation
Issuing agency(ies) State Administration of Markets and China National Standardization Administration
Summary This standard specifies the method for determining the tensile strength, elongation at break, crack length and tensile energy absorption of paper and paperboard using a test instrument with constant tensile speed (20 mm/min), and specifies the tensile index, The calculation formula of tensile energy absorption index and elastic modulus. This standard applies to all paper and board except corrugated board.

BASIC DATA
Standard ID GB/T 12914-2008 (GB/T12914-2008)
Description (Translated English) Paper and board. Determination of tensile properties
Sector / Industry National Standard (Recommended)
Classification of Chinese Standard Y30
Classification of International Standard 85-010
Word Count Estimation 13,172
Date of Issue 2008-08-19
Date of Implementation 2009-05-01
Older Standard (superseded by this standard) GB/T 12914-1991; GB/T 453-2002
Quoted Standard GB/T 450; GB/T 451.2; GB/T 451.3; GB/T 10739
Adopted Standard ISO 1924-1-1992, MOD; ISO 1954-2-1994, MOD
Drafting Organization China Pulp and Paper Research Institute
Administrative Organization National Standardization Technical Committee Paper Industry
Regulation (derived from) National Standard Approval Announcement 2008 No.14 (Total No.127)
Proposing organization China Light Industry Federation
Issuing agency(ies) Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China; Standardization Administration of China
Summary This standard specifies the paper and cardboard measuring the tensile strength of two methods: Constant loading method and the constant speed stretching. This standard applies to all paper and cardboard corrugated board except outside.

BASIC DATA
Standard ID GB/T 12914-1991 (GB/T12914-1991)
Description (Translated English) Paper and board--Determination of tensile properties--Constant rate of elongation method
Sector / Industry National Standard (Recommended)
Classification of Chinese Standard Y32
Classification of International Standard 85.06
Word Count Estimation 7,750
Date of Issue 1991/5/18
Date of Implementation 1992/3/1
Quoted Standard GB 450; GB/T 451.2; GB 453; GB 3358
Adopted Standard ISO 1924-2-1985, MOD
Regulation (derived from) Announcement of Newly Approved National Standards 2008 No. 14 (No. 127 overall)
Proposing organization People Republic of China Ministry of Light Industry
Issuing agency(ies) State Bureau of Technical Supervision