GB/T 23364.6-2009: Methods for chemical analysis of high purity indium oxide -- Part 6: Determination of the loss on ignition -- Gravimetric analysis
Status: Valid
Standard IDUSDBUY PDFLead-DaysStandard Title (Description)Status
GB/T 23364.6-2009149 Add to Cart 2 days Methods for chemical analysis of high purity indium oxide -- Part 6: Determination of the loss on ignition -- Gravimetric analysis Valid

Similar standards

GB/T 39859   GB/T 20892   GB/T 23513.1   GB/T 23364.3   GB/T 23364.4   GB/T 23364.2   

Basic data

Standard ID: GB/T 23364.6-2009 (GB/T23364.6-2009)
Description (Translated English): Methods for chemical analysis of high purity indium oxide -- Part 6: Determination of the loss on ignition -- Gravimetric analysis
Sector / Industry: National Standard (Recommended)
Classification of Chinese Standard: H66
Classification of International Standard: 77.120
Word Count Estimation: 5,525
Date of Issue: 2009-03-19
Date of Implementation: 2010-01-01
Regulation (derived from): National Standard Approval Announcement 2009 No.3 (Total No.143)
Issuing agency(ies): General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, Standardization Administration of the People's Republic of China
Summary: This standard specifies the determination of high-purity indium oxide loss on ignition. This section applies to the determination of high-purity indium oxide loss on ignition. Measuring range (mass fraction) of 0. 05% to 1. 00%.

GB/T 23364.6-2009: Methods for chemical analysis of high purity indium oxide -- Part 6: Determination of the loss on ignition -- Gravimetric analysis


---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order.
Methods for chemical analysis of high purity indium oxide Part 6. Determination of the loss on ignition Gravimetric analysis. ICS 77.120 H66 National Standards of People's Republic of China Methods for chemical analysis of high purity indium oxide Part 6. Determination of loss on ignition weighing method Posted 2009-03-19 2010-01-01 implementation Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China Standardization Administration of China released

Foreword

GB/T 23364 "Methods for chemical analysis of high purity indium oxide" is divided into six sections. --- Part 1. Determination of arsenic content by atomic fluorescence spectrometry; --- Part 2. Determination of tin content of phenyl spectrophotometric; --- Part 3. Determination of antimony content - Atomic Fluorescence Spectrometry; --- Part 4. aluminum, iron, copper, zinc, cadmium, lead and thallium content - Inductively Coupled Plasma Mass Spectrometry; --- Part 5. Determination of chlorine content of thiocyanate mercury spectrophotometry; --- Part 6. Determination of loss on ignition weighing method. Part is divided into 6 sections. This part is proposed by the China Nonferrous Metals Industry Association. The non-ferrous metal part by the National Standardization Technical Committee. This in part by the Guilin Institute of Technology, China Nonferrous Metals Industry Institute of Standards Metrology and Quality is responsible for drafting. This part by the Guangxi metallurgical products Quality Supervision, Inspection Station, indium Industry Association Guangxi Liuzhou product quality supervision, inspection and participated in the drafting. The main drafters of this section. Zhou Sulian, Huangzhao Min, Huang Xusheng, Liaoqing Wen, Ling Palace oct, Wuxiang Wu, Wei Li, Wang Ying. Methods for chemical analysis of high purity indium oxide Part 6. Determination of loss on ignition weighing method

1 Scope

This section GB/T 23364 specifies the method for determination of loss on ignition of high-purity indium oxide. This section applies to the determination of loss on ignition of high-purity indium oxide, measurement range (mass fraction) of 0.05% to 1.00%.

2 Method summary

Sample was placed in a platinum crucible at a high temperature furnace is gradually heated up to 800 ℃, burning to constant calculated based on the loss on ignition which reduces quality.

3 Equipment

3.1 Analysis of balance. a sense of the amount of 0.1mg. 3.2 high-temperature furnace.

4 Sample

The specimen should be 105 ℃ ~ 110 ℃ drying 2h, placed in a desiccator to cool to room temperature. Step 5 Analysis 5.1 Sample Weigh 3.00g sample, accurate to 0.0001g. 5.2 Determination of the number of Independently measured twice and averaged. 5.3 Determination 5.3.1 The sample (5.1) were plated at 800 ℃ constant burning and has a platinum crucible (including platinum cover) in. 5.3.2 platinum crucible placed in a high temperature furnace was slowly heated to 800 ℃, burning 1h. 5.3.3 Remove the platinum crucible, coolish. The platinum crucible placed in a desiccator, cooled to room temperature and weigh. 5.3.4 platinum crucible placed in a high temperature furnace again, burning at 800 ℃ 30min. 5.3.3 according to the following operation until the constant. Calculation results of the analysis of 6 Ignition loss mass fraction w1 and its value is expressed in%, according to formula (1). W1 m1 = m1 2 m1 0 × 1- 100 (1) Where. M1 --- before burning sample and a platinum crucible (including platinum cover) mass in grams (g); M1 2 --- after burning a sample and a platinum crucible (including platinum cover) mass in grams (g); 0 --- mass m1 of sample in grams (g).

7 precision

7.1 Repeatability Found two independent test results obtained under repeatability conditions within the average range given below, these two test results
......
Image     

Tips & Frequently Asked Questions:

Question 1: How long will the true-PDF of GB/T 23364.6-2009_English be delivered?

Answer: Upon your order, we will start to translate GB/T 23364.6-2009_English as soon as possible, and keep you informed of the progress. The lead time is typically 1 ~ 2 working days. The lengthier the document the longer the lead time.

Question 2: Can I share the purchased PDF of GB/T 23364.6-2009_English with my colleagues?

Answer: Yes. The purchased PDF of GB/T 23364.6-2009_English will be deemed to be sold to your employer/organization who actually pays for it, including your colleagues and your employer's intranet.

Question 3: Does the price include tax/VAT?

Answer: Yes. Our tax invoice, downloaded/delivered in 9 seconds, includes all tax/VAT and complies with 100+ countries' tax regulations (tax exempted in 100+ countries) -- See Avoidance of Double Taxation Agreements (DTAs): List of DTAs signed between Singapore and 100+ countries

Question 4: Do you accept my currency other than USD?

Answer: Yes. If you need your currency to be printed on the invoice, please write an email to Sales@ChineseStandard.net. In 2 working-hours, we will create a special link for you to pay in any currencies. Otherwise, follow the normal steps: Add to Cart -- Checkout -- Select your currency to pay.