YS/T 861.5-2013 English PDFUS$159.00 · In stock
Delivery: <= 3 days. True-PDF full-copy in English will be manually translated and delivered via email. YS/T 861.5-2013: Methods for chemical analysis of niobium-titanium alloy. Part 5: Determination of titanium content-The ammonium ferric sulfate titration Status: Valid
Basic dataStandard ID: YS/T 861.5-2013 (YS/T861.5-2013)Description (Translated English): Methods for chemical analysis of niobium-titanium alloy. Part 5: Determination of titanium content-The ammonium ferric sulfate titration Sector / Industry: Nonferrous Metallurgy Industry Standard (Recommended) Classification of Chinese Standard: H63 Classification of International Standard: 77.120.99 Word Count Estimation: 6,621 Regulation (derived from): Ministry of Industry and Information Technology Bulletin 2013 No. 23; industry standard filing Notice 2013 No. 7 (No. 163 overall) Issuing agency(ies): Ministry of Industry and Information Technology Summary: This standard specifies the amount of niobium- titanium alloy method. This standard applies to the determination of the amount of niobium- titanium alloy, measuring range 40. 00% ~ 60. 00%. YS/T 861.5-2013: Methods for chemical analysis of niobium-titanium alloy. Part 5: Determination of titanium content-The ammonium ferric sulfate titration---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order. Methods for chemical analysis of niobium-titanium alloy Part 5. Determination of titanium content-The ammonium ferric sulfate titration ICS 77.120.99 H63 People's Republic of China Nonferrous Metals Industry Standard Niobium-titanium alloys Part 5. Determination of titanium content Ammonium ferric sulfate titration Part 5. Determinationoftitaniumcontent- Issued on. 2013-04-25 2013-09-01 implementation Ministry of Industry and Information Technology of the People's Republic of China released ForewordYS/T 861 "niobium-titanium alloy chemical analysis method" is divided into five sections. --- Part 1. aluminum, nickel, silicon, iron, chromium, copper, tantalum content - Inductively coupled plasma atomic emission spectrometry; --- Part 2. oxygen, the determination of nitrogen inert gas fusion infrared absorption/thermal conductivity method; --- Part 3. Determination of hydrogen content of inert gas fusion thermal conductivity method; --- Part 4. Determination of carbon content in the high-frequency combustion infrared absorption method; --- Part 5. Determination of the amount of titanium ammonium ferric sulfate titration. This section YS/T 861 Part 5. This section drafted in accordance with GB/T 1.1-2009 given rules. The non-ferrous metal part by the National Standardization Technical Committee (SAC/TC243) centralized. This section is drafted. Western Metal Materials Co., Ltd., Northwest Nonferrous Metal Research Institute, Beijing Nonferrous Metal Research Institute. The main drafters of this section. Zhang Bin, Li Tuo, Zhai through Germany, floating Haixia, Zhou Jinzhi, Jiang Yanni, Sunbao Lian, Zhou Kai, Li Bo, Liu. Niobium-titanium alloys Part 5. Determination of titanium content Ammonium ferric sulfate titration1 ScopeYS/T 861 This part provides for determination of niobium-titanium alloy titanium content. This section applies to the determination of niobium-titanium alloy titanium content, measurement range 40.00% ~ 60.00%.2 Method summaryHydrofluoric acid, nitric acid decomposition of the sample, niobium citrate complex. 20% to 30% sulfuric acid medium, under an inert atmosphere protected with aluminum foil Titanium (Ⅳ) reduction of titanium (Ⅲ), potassium thiocyanate as indicator, titration solution titrated with ammonium ferric sulfate standard.3 ReagentsUnless otherwise indicated, this part of the reagents were analytical reagent, which is a water or equivalent purity water. 3.1 sulfate (ρ = 1.84g/mL). 3.2 sulfate (11). 3.3 Hydrofluoric acid (ρ = 1.15g/mL). 3.4 nitric acid (ρ = 1.42g/mL). 3.5 citric acid solution. 400g/L. 3.6 saturated sodium bicarbonate solution. 3.7 Foil (mass fraction ≥99.95%). 3.8 Potassium thiocyanate solution. 250g/L. 3.9 ammonium ferric sulfate. 3.10 Titanium standard stock solution. Weigh 1.0000g of titanium (mass fraction ≥99.99%) in 500mL beaker covered with a watch glass, 100mL was added sulfuric acid (3.2), low-temperature heating the titanium is completely dissolved, was added dropwise nitric acid (3.4) until the solution is colorless, driving micro-boiling nitrogen oxides. Cooled and transferred to 1000mL volumetric flask, dilute with water to volume, and mix. This solution 1mL containing 1.0mg titanium. 3.11 ammonium ferric sulfate standard titration solution. about 0.02mol/L. 3.11.1 preparation. Weigh 48g of ammonium ferric sulfate (3.9) in 2000mL beaker, 500mL of water, sulfuric acid was slowly added 250mL (3.1), low temperature Heated to dissolve, cooled and transferred to 5000mL reagent bottle, dilute with water to volume, and mix. 3.11.2 Calibration. Pipette three 20.00mL titanium standard solution (3.10), respectively, 500mL Erlenmeyer flask, add 90mL water, according to the following points 5.4.2 Analysis steps. (3.11) very poor value volume of ammonium ferric sulfate standard titration solution consumed parallel calibration should not exceed 0.10mL, whichever average value. While doing the blank test. According to equation (1) Calculation Titration factor. ......Tips & Frequently Asked Questions:Question 1: How long will the true-PDF of YS/T 861.5-2013_English be delivered?Answer: Upon your order, we will start to translate YS/T 861.5-2013_English as soon as possible, and keep you informed of the progress. The lead time is typically 1 ~ 3 working days. The lengthier the document the longer the lead time.Question 2: Can I share the purchased PDF of YS/T 861.5-2013_English with my colleagues?Answer: Yes. The purchased PDF of YS/T 861.5-2013_English will be deemed to be sold to your employer/organization who actually pays for it, including your colleagues and your employer's intranet.Question 3: Does the price include tax/VAT?Answer: Yes. Our tax invoice, downloaded/delivered in 9 seconds, includes all tax/VAT and complies with 100+ countries' tax regulations (tax exempted in 100+ countries) -- See Avoidance of Double Taxation Agreements (DTAs): List of DTAs signed between Singapore and 100+ countriesQuestion 4: Do you accept my currency other than USD?Answer: Yes. If you need your currency to be printed on the invoice, please write an email to Sales@ChineseStandard.net. In 2 working-hours, we will create a special link for you to pay in any currencies. Otherwise, follow the normal steps: Add to Cart -- Checkout -- Select your currency to pay. |