Home Cart Quotation About-Us
www.ChineseStandard.net
SEARCH

YS/T 738.4-2010 English PDF

US$179.00 · In stock
Delivery: <= 2 days. True-PDF full-copy in English will be manually translated and delivered via email.
YS/T 738.4-2010: Analysis method for aluminum hydroxide for filler. Part 4: Determination method of viscosity
Standard IDUSDBUY PDFLead-DaysStandard Title (Description)Status
YS/T 738.4-2010179 Add to Cart 2 days Analysis method for aluminum hydroxide for filler. Part 4: Determination method of viscosity  

Similar standards

GB/T 1425   GB/T 351   YS/T 581.2   YS/T 581.15   YS/T 738.5   YS/T 738.3   

Basic data

Standard ID: YS/T 738.4-2010 (YS/T738.4-2010)
Description (Translated English): Analysis method for aluminum hydroxide for filler. Part 4: Determination method of viscosity
Sector / Industry: Nonferrous Metallurgy Industry Standard (Recommended)
Classification of Chinese Standard: H21
Classification of International Standard: 87.060.10
Word Count Estimation: 5,510
Date of Issue: 2010-11-22
Date of Implementation: 2011-03-01
Regulation (derived from): MIIT (2010) No. 126
Issuing agency(ies): Ministry of Industry and Information Technology
Summary: This standard specifies the filler aluminum hydroxide Determination of the viscosity. This standard applies to aluminum hydroxide for filler viscosity. Measuring range: 1500MPa �� s ~ 80000MPa �� S.

YS/T 738.4-2010: Analysis method for aluminum hydroxide for filler. Part 4: Determination method of viscosity


---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order.
Analysis method for aluminum hydroxide for filler.Part 4. Determination method of viscosity ICS 87.060.10 H21 People's Republic of China Nonferrous Metals Industry Standard Analysis of aluminum hydroxide filler Determination of the viscosity. Part 4 Part 4. Determinationmethodofviscosity Issued on. 2010-11-22 2011-03-01 implementation Ministry of Industry and Information Technology of the People's Republic of China released

Foreword

YS/T 738 "filler aluminum hydroxide analysis method" is divided into four parts. --- Part 1. Determination of pH; --- Part 2. Determination of soluble alkali content; --- Part 3. Determination of sulfide content; --- Part 4. Determination of viscosity. This is Part 4. This section drafted in accordance with GB/T 1.1-2009 given rules. The non-ferrous metal part by the National Standardization Technical Committee (SAC/TC243) centralized. This part of the Aluminum Corporation of China Shandong Branch, China Nonferrous Metals Industry Institute of Standards Metrology and Quality is responsible for drafting. This section drafted by the Aluminum Corporation of China Shandong Branch. The main drafters of this section. Wang Jingwei, Yang Zhihua Xu good text, Zhaisheng Chang. Analysis of aluminum hydroxide filler Determination of the viscosity. Part 4

1 Scope

YS/T of the provisions of section 738 of the measurement method using aluminum hydroxide filler viscosity. This section applies to the filler aluminum hydroxide viscosity measurement. Measuring range. 1500MPa · s ~ 80000MPa · s.

2 principle of the method

Simulation of aluminum hydroxide filler during actual use of the epoxy resin mix, after incubation, with a viscometer mixed slurry Viscosity.

3 Instruments and reagents

3.1 Epoxy. 850S. 3.2 dryer. 3.3 thermostatic water tank. 3.4 glass rod. 3.5 viscometer. 3.6 Balance. a sense of the amount of 0.1g. 3.7 plastic cup. 300mL.

4 Sample

The sample was placed in a closed container, the capacity of the container to be almost full sample is appropriate. Step 5 Analysis 5.1 Sample Weigh first epoxy resin (3.1) 60g, and then weighed sample (4) 90g, placed in plastic cups (3.7) in. 5.2 Determination of the number of Independently measured twice and averaged. 5.3 Determination A sample (5.1) was stirred 5min mix with a glass rod (3.4), placed in 40 ℃ constant temperature water bath (3.3) and incubated 30min, a viscosity Measured, 5min after record readings.
......
Image     

Tips & Frequently Asked Questions:

Question 1: How long will the true-PDF of YS/T 738.4-2010_English be delivered?

Answer: Upon your order, we will start to translate YS/T 738.4-2010_English as soon as possible, and keep you informed of the progress. The lead time is typically 1 ~ 2 working days. The lengthier the document the longer the lead time.

Question 2: Can I share the purchased PDF of YS/T 738.4-2010_English with my colleagues?

Answer: Yes. The purchased PDF of YS/T 738.4-2010_English will be deemed to be sold to your employer/organization who actually pays for it, including your colleagues and your employer's intranet.

Question 3: Does the price include tax/VAT?

Answer: Yes. Our tax invoice, downloaded/delivered in 9 seconds, includes all tax/VAT and complies with 100+ countries' tax regulations (tax exempted in 100+ countries) -- See Avoidance of Double Taxation Agreements (DTAs): List of DTAs signed between Singapore and 100+ countries

Question 4: Do you accept my currency other than USD?

Answer: Yes. If you need your currency to be printed on the invoice, please write an email to Sales@ChineseStandard.net. In 2 working-hours, we will create a special link for you to pay in any currencies. Otherwise, follow the normal steps: Add to Cart -- Checkout -- Select your currency to pay.