YS/T 461.2-2013 English PDF

US$189.00 · In stock
Delivery: <= 3 days. True-PDF full-copy in English will be manually translated and delivered via email.
YS/T 461.2-2013: Methods for chemical analysis of lead and zinc bulk concentrates. Part 2: The determination of iron content. Na2EDTA titrimetric method
Status: Valid

YS/T 461.2: Historical versions

Standard IDUSDBUY PDFLead-DaysStandard Title (Description)Status
YS/T 461.2-2013189 Add to Cart 3 days Methods for chemical analysis of lead and zinc bulk concentrates. Part 2: The determination of iron content. Na2EDTA titrimetric method Valid
YS/T 461.2-2003239 Add to Cart 2 days The methods for chemical analysis of lead and zinc bulk concentrates-The determination of iron content-The Na_2EDTA titrmetric method Obsolete

Similar standards

GB/T 3884.2   GB/T 3884.1   YS/T 521.2   YS/T 461.11   YS/T 461.1   YS/T 461.10   

Basic data

Standard ID: YS/T 461.2-2013 (YS/T461.2-2013)
Description (Translated English): Methods for chemical analysis of lead and zinc bulk concentrates. Part 2: The determination of iron content. Na2EDTA titrimetric method
Sector / Industry: Nonferrous Metallurgy Industry Standard (Recommended)
Classification of Chinese Standard: H13
Classification of International Standard: 77.120.60
Word Count Estimation: 7,742
Older Standard (superseded by this standard): YS/T 461.2-2003
Regulation (derived from): Ministry of Industry and Information Technology Bulletin No. 52, 2013; industry standard for filing Notice No. 1 of 2014 (No. 169 overall)
Issuing agency(ies): Ministry of Industry and Information Technology
Summary: This standard specifies the method for the determination of lead and zinc concentrates mixed iron content. This standard applies to the determination of the iron content of lead and zinc concentrates mixed. Measuring range: 2. 00% to 20. 00%. This standar

YS/T 461.2-2013: Methods for chemical analysis of lead and zinc bulk concentrates. Part 2: The determination of iron content. Na2EDTA titrimetric method


---This is a DRAFT version for illustration, not a final translation. Full copy of true-PDF in English version (including equations, symbols, images, flow-chart, tables, and figures etc.) will be manually/carefully translated upon your order.
Methods for chemical analysis of lead and zinc bulk concentrates Part 2. The determination of iron content Na2EDTA titrimetric method. ICS 77.120.60 H13 People's Republic of China Nonferrous Metals Industry Standard Replacing YS/T 461.2-2003 Lead and Zinc concentrates - Methods Part 2. Determination of iron content Na2EDTA titration Part 2. Thedeterminationofironcontent- Issued on. 2013-10-17 2014-03-01 implementation Ministry of Industry and Information Technology of the People's Republic of China released

Foreword

YS/T 461 "Lead and Zinc concentrates - Methods" is divided into 11 parts. --- Part 1. Determination of the amount of lead and zinc content Na2EDTA precipitation titration; --- Part 2. Determination of iron content Na2EDTA titration; --- Part 3. Determination of sulfur content of combustion - neutralization titration method; --- Part 4. Determination of arsenic content of iodine titration; --- Part 5. Determination of silicon dioxide content - Molybdenum blue spectrophotometric method; --- Part 6. Determination of the amount of mercury atomic fluorescence spectrometry; --- Part 7. Determination of cadmium content by flame atomic absorption spectrometry; --- Part 8. Determination of copper content - Flame atomic absorption spectrometry; --- Part 9. Determination of the amount of silver by flame atomic absorption spectrometry; --- Part 10. the amount of gold and silver contents - fire assay; --- Part 11. arsenic, bismuth, cadmium, cobalt, copper, nickel, antimony content - Inductively Coupled Plasma - Atomic Emission Spectrometry. This section YS/T Part 2 461. This section drafted in accordance with GB/T 1.1-2009 given rules. The partial replacement of YS/T 461.2-2003 "Lead and Zinc concentrates - Determination of iron content Na2EDTA titration" Compared with YS/T 461.2-2003, the main changes are as follows. --- On the "analysis step" clause in the sample dissolution method was modified; --- Added "reproducibility" clause, delete the words "to allow poor" clause; --- Added "the test report" requirement. The non-ferrous metal part by the National Standardization Technical Committee (SAC/TC243) centralized. YS/T 461 is responsible for drafting. Shenzhen Lingnan Nonferrous Metals Co., Baiyin Nonferrous Metals Corporation, Beijing Institute of Mining and Metallurgy. This section is responsible for drafting. Shenzhen Lingnan Nonferrous Metals Co. Fankou. Participated in the drafting of this section. Shenzhen Lingnan Nonferrous Metals Co., Ltd. Shaoguan smelter Baiyin Nonferrous Metals Group Limited shares The company, Western Mining Corporation and Inspection Center, Western Mining xitiesan branch. The main drafters of this section. Xie Huiyuan, Yan Bin, Lin Ye, Wang Dongzhen, Wang, Yang Zhanju, Wang, Lung Ying-Lan, Du Feng, Li Li. This part of the standard replaces the previous editions are. --- YS/T 461.2-2003. Lead and Zinc concentrates - Methods Part 2. Determination of iron content Na2EDTA titration

1 Scope

This section YS/T 461 specifies the method for determination of Lead and Zinc concentrate iron content. This section applies to the determination of Lead and Zinc concentrate iron content. Measuring range. 2.00% to 20.00%. This section does not apply to bismuth content of more than 0.3% Lead and Zinc concentrate.

2 Method summary

Sample was dissolved with hydrochloric acid, nitric acid, sulfuric acid, nitric acid and evaporated to dryness to remove low. Dissolved salts with hydrochloric acid, add ammonia iron precipitated as ferric hydroxide, Filtration, separation coexisting elements. Dissolve the precipitate with dilute hydrochloric acid and acidity regulator in micro-boiling conditions to sulfosalicylic acid as an indicator to Na2EDTA standard titration solution titration to the solution from purple to bright yellow as the end point. According to standard titration solution consumed Na2EDTA The calculation of the volume of the iron content.

3 Reagents

Unless otherwise indicated in the analysis using only recognized as analytical grade reagents and distilled or deionized water or equivalent purity. 3.1 ammonium chloride. 3.2 hydrochloric acid (ρ = 1.19g/mL). 3.3 nitric acid (ρ = 1.42g/mL). Aqueous ammonia 3.4 (ρ = 0.90g/mL). 3.5 sulfate (ρ = 1.84g/mL). 3.6 hydrochloride (11). 3.7 hydrochloride (110). 3.8 Aqueous ammonia (11). 3.9 ammonium fluoride solution (250g/L). 3.10 ammonium chloride bath. Weigh 25g ammonium chloride (3.1) were dissolved in 500mL of water, add 20mL ammonia (3.4), and mix. 3.11 Sulfosalicyl indicator (100g/L). 3.12 disodium edetate (Na2EDTA) standard titration solution. 3.12.1 preparation. Weigh 10gNa2EDTA (C10H14N2O8Na2 · 2H2O) in 400mL beaker was added 200mL of water, heating solution Solution is completely cooled to room temperature and transferred to 1000mL volumetric flask, dilute with water to volume, and mix. Calibration after placing 3d. 3.12.2 Calibration. Weigh 0.060g (accurate to 0.0001g) pre-drying at 105 ℃ ± 5 ℃ oven 1h, cooled and placed in a desiccator To room temperature and the iron oxide reference material in 300mL beaker, wetted with a small amount of water, plus 10mL of hydrochloric acid (3.2), purged with a small amount of water table Side dish and cup wall, low temperature heating steam until nearly dry. Add 2mL of hydrochloric acid (3.6) dissolved salts, water was added to 120mL, with aqueous ammonia (3.4) and the hydrogen to Iron oxide precipitate has just appeared, plus 8mL hydrochloric acid (3.7), heated to near boiling, remove it. Add 1mL Sulfosalicyl indicator (3.11), with Na2EDTA standard titration solution titration to the solution from purple to bright yellow is the end. Along with the calibration blank test.
......
Image     

Tips & Frequently Asked Questions:

Question 1: How long will the true-PDF of YS/T 461.2-2013_English be delivered?

Answer: Upon your order, we will start to translate YS/T 461.2-2013_English as soon as possible, and keep you informed of the progress. The lead time is typically 1 ~ 3 working days. The lengthier the document the longer the lead time.

Question 2: Can I share the purchased PDF of YS/T 461.2-2013_English with my colleagues?

Answer: Yes. The purchased PDF of YS/T 461.2-2013_English will be deemed to be sold to your employer/organization who actually pays for it, including your colleagues and your employer's intranet.

Question 3: Does the price include tax/VAT?

Answer: Yes. Our tax invoice, downloaded/delivered in 9 seconds, includes all tax/VAT and complies with 100+ countries' tax regulations (tax exempted in 100+ countries) -- See Avoidance of Double Taxation Agreements (DTAs): List of DTAs signed between Singapore and 100+ countries

Question 4: Do you accept my currency other than USD?

Answer: Yes. If you need your currency to be printed on the invoice, please write an email to Sales@ChineseStandard.net. In 2 working-hours, we will create a special link for you to pay in any currencies. Otherwise, follow the normal steps: Add to Cart -- Checkout -- Select your currency to pay.

Question 5: Should I purchase the latest version YS/T 461.2-2013?

Answer: Yes. Unless special scenarios such as technical constraints or academic study, you should always prioritize to purchase the latest version YS/T 461.2-2013 even if the enforcement date is in future. Complying with the latest version means that, by default, it also complies with all the earlier versions, technically.