YC/T 147-2023 (YC/T147-2023, YCT 147-2023, YCT147-2023) & related versions
YC/T 147-2023: PDF in English (YCT 147-2023) YC/T 147-2010
TOBACCO INDUSTRY STANDARD OF
THE PEOPLE’S REPUBLIC OF CHINA
ICS 65.160
X 87
Record No.: 30420-2011
Replacing YC/T 147-2001
Threshed tobacco - Quality inspection
ISSUED ON: DECEMBER 01, 2010
IMPLEMENTED ON: JANUARY 01, 2011
Issued by: State Tobacco Monopoly Administration
Table of Contents
Foreword ... 3
1 Scope ... 5
2 Normative references ... 5
3 Technical requirements ... 6
4 Testing of moisture content ... 8
5 Testing of lamina structure ... 9
6 Testing of debris and detritus structures ... 10
7 Testing of stem content in lamina ... 11
8 Testing of density deviation rate in box (DVR) ... 11
9 Testing of main chemical composition ... 12
10 Testing of long stem content ... 13
11 Testing of lamina (detritus) content in stem ... 14
12 Mass testing ... 15
13 Testing of sundries ... 15
14 Testing of appearance ... 16
15 Comprehensive determination ... 17
Threshed tobacco - Quality inspection
1 Scope
This Standard specifies inspection methods and determination for quality of
tobacco leaf lamina, stem, debris and detritus (finished production) after
threshing and redrying.
This Standard is applicable to flue-cured tobacco and burley tobacco.
2 Normative references
The following referenced documents are indispensable for the application of
this document. For dated references, only the edition cited applies. For undated
references, the latest edition of the referenced document (including any
amendments) applies.
GB/T 21136, Threshed tobacco - Determination of stem content
GB/T 21137, Leaf tobacco - Determination of strip particle size
YC/T 31, Tobacco and tobacco products - Preparation of test sample and
determination of water content - Oven method
YC/T 137.1, Package of redried strip - Corrugated carton
YC/T 146, Leaf tobacco - Threshing and redrying - Technical specification
YC/T 159, Tobacco and tobacco products - Determination of water soluble
sugars - Continuous flow method
YC/T 160, Tobacco and tobacco products - Determination of total alkaloids-
Continuous flow method
YC/T 161, Tobacco and tobacco products - Determination of total nitrogen-
Continuous flow method
YC/T 162, Tobacco and tobacco products - Determination of chloride -
Continuous flow method
YC/T 217, Tobacco and tobacco products - Determination of Potassium -
Continuous flow method
YC/T 236, Tobacco and tobacco products - Nondestructive detection of strip
according to 2 boxes (bales). The space between the two sample boxes shall
be more than 20. After opening 15cm~20cm thick laminas, diagonally at the
quarter point, respectively take 30g~40g of samples. After mixing, put into a
sample container. Seal and store. Mark for spare use.
4.1.2 Samples of stem, debris and detritus
In the finished product warehouse, sample according to 2% for products of
same lot and same grade. When it is less than 100 boxes (bales), sample
according to 2 boxes (bales). The space between the two sample boxes shall
be more than 20. Then use a sampler to cut out 10cm~20cm thick tobacco stem,
debris and detritus. Extract about 100g of sample in each sample box (bale).
Respectively put into a sample container. Seal and store. Mark for spare use.
4.2 Testing of moisture content
4.2.1 Sample crushing
Start the grinder. After preheating by rotating mechanical friction, crush the
sample into smoke powder with a size less than 3mm. Dispense the crushed
smoke powder and put into a sample container. Immediately seal and mark.
Before crushing the sample, clean each component of the grinder, without any
pollution.
4.2.2 Testing of moisture content
In accordance with YC/T 31.
4.3 Determination
If the moisture content of sample meets the technical requirements in 3.1, it
shall determine that the moisture content indicator of this sample is conforming;
otherwise it shall be nonconforming. If the acceptability of the moisture content
indicator of this lot of products is greater than 95%, it shall determine that the
moisture content indicator of this lot of products is conforming; otherwise it shall
be nonconforming.
5 Testing of lamina structure
5.1 Sample preparation
In the finished product warehouse, sample according to 2% for products of
same lot and same grade. When it is less than 100 boxes, sample according to
2 boxes. The space between the two sample boxes shall be more than 20. Lift
up the strips with a thickness of about 10cm~20cm of the upper layer tobacco
box in one go. Then extract the whole piece of the strip. Each portion is
(3000±300)g. Respectively load into the sample container. Mark for spare use.
5.2 Testing of lamina structure
In accordance with GB/T 21137.
5.3 Determination
If the lamina structure of sample meets technical requirements of 3.1, it shall
determine that the lamina structure indicator of this sample is conforming;
otherwise it shall be nonconforming. If the acceptability of the lamina structure
indicator of this lot of products is greater than 85%, it shall determine that the
lamina structure indicator of this lot of products is conforming; otherwise it shall
be nonconforming.
6 Testing of debris and detritus structures
6.1 Sample preparation
In the finished product warehouse, sample according to 2% for products of
same lot and same grade. When it is less than 100 boxes, sample according to
3 boxes. The space between the two sample boxes shall be more than 20. Then
use a sampler to push aside 10cm~20cm thick debris and detritus on the
surface. Extract 100g~150g of samples in each sample box (or sack).
Respectively put into the sample container. Seal to store. Mark for spare use.
6.2 Instruments
6.2.1 Circular oscillation sorting sieve
When determining debris, use sieves of which clear bore diameters are Φ5mm,
Φ4mm, Φ3mm. When determining detritus, use sieves of which clear bore
diameters are Φ2mm, Φ1mm, Φ0.71mm.
6.2.2 Electronic scale
The resolution is 0.1g.
6.3 Operating steps
Pour all samples onto the circular oscillation sorting sieve. Vibrate 5min. Collect
samples at each grade of sieves. Respectively weigh their masses.
6.4 Calculation
Calculate the content of a specification of debris or detritus according to formula
In the finished product warehouse, sample according to 0.2% for products of
same lot and same grade. When it is less than 500 boxes, sample according to
1 box. The space between the two sample boxes shall be more than 200.
8.2 Testing method
In accordance with YC/T 236.
8.3 Determination
If the DVR indicator of sample meets technical requirements in 3.1, it shall
determine that the DVR indicator of this sample is conforming; otherwise it shall
be nonconforming. If the acceptability of the DVR indicators of this lot of
products is greater than 85%, it shall determine that the DVR indicators of this
lot of products are conforming; otherwise they shall be nonconforming.
9 Testing of main chemical composition
9.1 Testing items
The chemical composition tested includes:
- Total carbohydrates;
- Nicotine;
- Total nitrogen;
- Chlorine (Cl);
- Potassium (K).
NOTE: Add testing items according to the contract requirements.
9.2 Sample preparation
Excess sample in 4.1.1 of this Standard.
9.3 Testing method
Test total carbohydrates, nicotine, total nitrogen, chlorine and potassium
according to the following methods:
- Total carbohydrates: in accordance with YC/T 159;
- Nicotine: in accordance with YC/T 160;
- Total nitrogen: in accordance with YC/T 161;
If the long stem content of sample meets technical requirements in 3.1, it shall
determine that the long stem content indicator of this sample is conforming;
otherwise it shall be nonconforming. If the acceptability of the long stem content
indicators of this lot of products is greater than 85%, it shall determine that the
long stem content indicators of this lot of samples is conforming; otherwise they
shall be nonconforming.
11 Testing of lamina (detritus) content in stem
11.1 Sample preparation
Extract 1000g~1500g of samples according to 4.1.2.
11.2 Electronic scale
The resolution is 0.1g.
11.3 Operation
Pour stem samples on the sample division plate to fully mix. Use the quarter
method to divide into 80g~120g. Tear off the laminas attached to the tobacco
stem. Collect all detritus under stem and weigh.
11.4 Calculation
Calculate the lamina (detritus) content in stem according to formula (4).
where,
X2 - Lamina (detritus) content in stem, %;
m3 - Masses of lamina and detritus attached in stem, in grams (g);
m4 - Sample mass, in grams (g).
11.5 Determination
If the lamina content in stem of sample meets technical requirements in 3.1, it
shall determine that the lamina content indicator in stem of this sample is
conforming; otherwise it shall be nonconforming. If the acceptability of the
lamina content indicators in stem of this lot of products is greater than 85%, it
shall determine that the lamina content indicators in stem of this lot of samples
is conforming; otherwise they shall be nonconforming.
- No oil and water stains;
- Lap is tight;
- The carton box is straight and intact;
- Straighten the strapping straps and arrange them evenly;
- The finished strip forming box rises no more than 50mm.
14.2.2 Sack packing shall meet the following requirements:
- See Table 6 for requirements of marks;
- The text is neatly arranged, the handwriting is clear, and no typographical
errors can occur;
- The package shall not be damaged and the tobacco stems shall not be
exposed;
- No oil and water stains.
14.3 Determination
If any two clauses of 14.2.1 or 14.2.2 are not met, the mark indicator of this box
(bale) of samples shall be nonconforming. If the acceptability of the mark
indicators of this lot of products is greater than 90%, it shall determine that the
mark indicators of this lot of products are conforming; otherwise they shall be
nonconforming.
15 Comprehensive determination
If all indicators are conforming, it shall determine that this lot of products are
conforming.
If any one of the primary indicators is nonconforming, it shall determine that this
lot of products are nonconforming.
If all the primary indicators are conforming, two or more secondary indicators
are nonconforming, it shall determine that this lot of products are
nonconforming.
If all primary indicators are conforming, one secondary indicator is
nonconforming, it shall double sampling for the nonconforming item to retest. If
this indicator during retest is conforming, it shall determine that this lot of
products are conforming. If this indicator during retest is nonconforming, it shall
determine that this lot of products are nonconforming.
......
Standard ID | YC/T 147-2023 (YC/T147-2023) | Description (Translated English) | Threshed tobacco - Quality requirements | Sector / Industry | Tobacco Industry Standard (Recommended) | Classification of Chinese Standard | X87 | Classification of International Standard | 65.160 | Word Count Estimation | 23,235 | Date of Issue | 2023-05-31 | Date of Implementation | 2023-08-01 | Older Standard (superseded by this standard) | YC/T 147-2010 | Drafting Organization | China Tobacco Leaf Corporation, Huahuan International Tobacco Co., Ltd., Guangdong Shaoguan Tobacco Leaf Recuring Co., Ltd., China Tobacco Standardization Research Center, Zhengzhou Tobacco Research Institute, Shanghai Tobacco Group Co., Ltd., Hubei Tobacco Golden Leaf Recuring Co., Ltd., Yunnan Tobacco Leaf Recuring Co., Ltd. Roasting Co., Ltd., Xianyang Tobacco Leaf Re-baking Co., Ltd., Jiangsu China Tobacco Industry Co., Ltd., Fujian Wuyi Tobacco Co., Ltd., Anhui China Tobacco Industry Co., Ltd., Fujian Longyan Golden Leaf Re-baking Co., Ltd., Hunan Tobacco Leaf Re-baking Co., Ltd., Hunan China Tobacco Industry Co., Ltd., Yunnan China Tobacco Industry Co., Ltd., Yunnan Tobacco Leaf Company, Shandong Tobacco Leaf Re-curing Co., Ltd., Tianchang International Tobacco Co., Ltd., Dandong Liaodong Tobacco Development Co., Ltd. | Administrative Organization | National Tobacco Standardization Technical Committee Technical Committee for Thinning and Recuring (SAC/TC 144/SC 13) | Proposing organization | State Tobacco Monopoly Administration | Issuing agency(ies) | State Tobacco Monopoly Administration |
|