GB/T 6730.68-2009English110 Add to Cart 0-9 seconds. Auto delivery. Iron ores -- Determination of loss on ignition -- Gravimetric method GB/T 6730.68-2009 Valid GBT 6730.68-2009
Buy with any currencies (Euro, JPY, KRW...): GB/T 6730.68-2009    Preview this PDF: GB/T 6730.68-2009



GB/T 6730.68-2009: PDF in English (GBT 6730.68-2009)
GB/T 6730.68-2009 GB NATIONAL STANDARD OF THE PEOPLE’S REPUBLIC OF CHINA ICS 73.060.10 D 31 Iron ores - Determination of loss on ignition - Gravimetric method ISSUED ON: OCTOBER 30, 2009 IMPLEMENTED ON: MAY 01, 2010 Issued by: General Administration of Quality Supervision, Inspection and Quarantine; Standardization Administration of the People's Republic of China. Table of Contents Foreword ... 3  1 Scope ... 4  2 Normative references ... 4  3 Terms and definitions ... 5  4 Principle ... 5  5 Reagents and materials ... 5  6 Equipment ... 5  7 Sampling and sample preparation ... 5  8 Analysis steps ... 6  9 Result calculation ... 6  10 Precision ... 7  11 Test report ... 7  Iron ores - Determination of loss on ignition - Gravimetric method WARNING - Persons using this Part of GB/T 6730 shall have experience in formal laboratory work. This Part does not address all security issues. It is the user's responsibility to take appropriate safety and health measures and to ensure compliance with the conditions stipulated by relevant national regulations. 1 Scope This Part of GB/T 6730 specifies determination of loss on ignition (LOI) in iron ore by gravimetric method. This Part is applicable to determination of ignition loss in natural iron ore, iron concentrate and sinter. The determination range (mass fraction): - 10.0%~12.0%. This Part does not apply to processed minerals containing metallic iron, natural or processed minerals with a sulfur content greater than 0.2% (mass fraction). 2 Normative references The following referenced documents are indispensable for the application of this part of GB/T 6730. For dated references, only the edition cited applies. For undated references, the latest edition of the referenced document (including any amendments) applies. GB/T 6379.2, Measurement methods and results - Accuracy (trueness and precision) - Part 2: Determine the standard methods of measurement repeatability and reproducibility of the basic method (GB/T 6379.2-2004, ISO 5725-2:1994, IDT) GB/T 6730.1, Iron ores - Preparation of pre-dried test samples for chemical analysis (GB/T 6730.1-1986, idt ISO 7764:1985) GB/T 8170, Rules of rounding off for numerical values and expression and judgement of limiting values GB/T 10322.1, Iron ores - Sampling and sample preparation procedures (GB/T 10322.1-2000, idt ISO 3082:1998) GB/T 20565, Iron ores and direct reduced iron - Vocabulary (GB/T 20565- 2006, ISO 11323:2002, IDT) 3 Terms and definitions The terms and definitions defined in GB/T 20565 apply to this Part. 4 Principle The test material is ignited to constant weight at 1000°C±25°C. Calculate the ignition loss based on the mass lost. 5 Reagents and materials Unless otherwise stated, only the confirmed analytically-pure reagents are used in the analysis. 5.1 Silica gel, dried at 105°C for 4h. 6 Equipment Laboratory routine equipment includes: 6.1 Porcelain crucible or platinum crucible: capacity is 15mL~25mL. 6.2 Balance: the sensitivity is 0.1mg. 6.3 High temperature furnace: the maximum operating temperature is not less than 1100°C, and can automatically control the temperature. 7 Sampling and sample preparation 7.1 Laboratory sample Samples for analysis shall be sampled and prepared according to GB/T 10322.1. Generally, the particle size of the specimen shall be less than 100μm. If the specimen has obvious burn loss (more than 2.0%), its particle size shall be less than 160μm. 7.2 Preparation of pre-dried specimens Mix the laboratory samples well. Use the increment method to sample. According to the provisions of GB/T 6730.1, the sample is dried at a temperature of 105°C±2°C. ......

BASIC DATA
Standard ID GB/T 6730.68-2009 (GB/T6730.68-2009)
Description (Translated English) Inon ores. Determination of loss on ignition. Gravimetric method
Sector / Industry National Standard (Recommended)
Classification of Chinese Standard D31
Classification of International Standard 73.060.10
Word Count Estimation 6,629
Date of Issue 2009-10-30
Date of Implementation 2010-05-01
Quoted Standard GB/T 6379.2; GB/T 6730.1; GB/T 8170; GB/T 10322.1; GB/T 20565
Drafting Organization Exit Inspection and Quarantine of the PRC Tianjin
Administrative Organization National Standardization Technical Committee of iron ore and direct reduced iron
Regulation (derived from) National Standard Approval Announcement 2009 No.12 (Total No.152)
Proposing organization China Iron and Steel Association
Issuing agency(ies) Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China; Standardization Administration of China
Summary This standard specifies the method for the determination of iron ore in the weight loss on ignition (LOI). This section applies to natural iron ore. Determination of iron ore reduction and sinter burning. Measuring range (mass fraction): -10. 0% to 12. 0%.