YY/T 1477.4-2017English150 Add to Cart 0--10 minutes. Auto immediate delivery. Standard test models for primary wound dressing performance evaluation—Part 4: In vitro wound model for adhesion properties evaluation of dressings Valid YY/T 1477.4-2017
YY/T 1477.4-2017Chinese16 Add to Cart <=1-day [PDF from Chinese Authority, or Standard Committee, or Publishing House]

  In 0~10 minutes time, full copy of this English-PDF will be auto-immediately delivered to your email. See samples for translation quality.  

BASIC DATA
Standard ID YY/T 1477.4-2017 (YY/T1477.4-2017)
Description (Translated English) Standard test models for primary wound dressing performance evaluation--Part 4: In vitro wound model for adhesion properties evaluation of dressings
Sector / Industry Medical Device & Pharmaceutical Industry Standard (Recommended)
Classification of Chinese Standard C48
Classification of International Standard 11.120.20
Word Count Estimation 10,112
Date of Issue 2017-02-28
Date of Implementation 2018-01-01
Drafting Organization Shandong Province Medical Device Quality Inspection Center, Minnesota Mining Manufacturing Medical Equipment (Shanghai) Co., Ltd., Shandong Saikesaisi Pharmaceutical Technology Co., Ltd.
Administrative Organization State Food and Drug Administration Jinan Medical Device Quality Supervision and Inspection Center
Regulation (derived from) China Food & Drug Administration Announcement 2017 No. 25
Proposing organization China Food and Drug Administration
Issuing agency(ies) State Food and Drug Administration

YY/T 1477.4-2017
YY
PHARMACEUTICAL INDUSTRY STANDARD
OF THE PEOPLE’S REPUBLIC OF CHINA
ICS 11.120.20
C 48
Standard test models for primary wound dressing
performance evaluation - Part 4. In vitro wound model
for adhesion properties evaluation of dressings
接触性创面敷料性能评价用标准试验模型
第 4部分. 评价创面敷料潜在粘连性的体外模型
ISSUED ON. FEBRUARY 28, 2017
IMPLEMENTED ON. JANUARY 1, 2018
Issued by. China Food and Drug Administration
Table of Contents
Foreword ... 3
Introduction ... 4
1 Scope ... 5
2 Terms and definitions ... 5
3 Summary... 5
4 Model construction ... 5
5 Model application ... 6
Appendix A (Informative) An example of a test using the wound model to
evaluate the potential adhesion of dressings ... 8
Appendix B (Informative) An example of a test using the wound model to
evaluate the performance between dressings ... 11
References ... 13
Standard test models for primary wound dressing
performance evaluation - Part 4. In vitro wound model
for adhesion properties evaluation of dressings
1 Scope
The in vitro wound model presented in this Part of YY/T 1477 is used to evaluate
and compare the potential adhesion properties of wound dressings in vitro.
This Part is applicable to the evaluation of the adhesion between the wound
contact layer of the dressing and the wound.
2 Terms and definitions
The following terms and definitions are applicable to this document.
2.1 Wound model
A fibrin clot which simulates a wound, to evaluate the potential adhesion
properties of the dressing to the wound.
3 Summary
This model is a unique in vitro quantitative model developed based on the
adhesion properties of wound dressings to fibrin clots. The water-soluble
fibrinogen is coagulated with thrombin into a water-insoluble fibrin, and further
solidified into a fibrin clot. An adhesion is provided by the protein clot, and the
wound is simulated with a biological matrix and applied between two dressings.
By measuring the peel force required to peel the dressing material from the
fibrin clot, the potential adhesion of the wound dressing is evaluated.
4 Model construction
4.1 Test devices
Test devices include.
a) 6-well cell culture plate (or other equivalent devices);
b) Constant temperature-humidity chamber;
c) Drying oven;
d) Precision balance with an accuracy of 0.001 g.
4.2 Preparation of wound model (fibrin clot)
4.2.1 Reagents
Reagents include.
a) Bovine serum albumin (BSA) phosphate buffer solution (c=10 mg/mL). 1.0
g of bovine serum albumin (BSA) is dissolved in 100 mL of phosphate
buffered saline (PBS);
b) Fibrinogen (source. cattle). commercially available;
c) Thrombin. USE an appropriate amount of 9 g/L sodium chloride solution
to dissolve, so that the concentration is about 300 units/mL.
4.2.2 Fibrin clot preparation
TAKE 3 g of fibrinogen; ADD it to bovine serum albumin (BSA) phosphate buffer
solution [4.2.1a)], so that the fibrinogen concentration is 30 mg/mL. Then, TAKE
10 mL of the solution and ADD to a 6-well cell culture plate; and ADD 1 mL of
thrombin to each well, and quickly MIX it well. The mixture is placed at (37±2)°C
for 1 h, and then cooled at room temperature for 1 h, to form and solidify a fibrin
clot.
Note. When fibrinogen is dissolved in the cold season or fibrinogen is just removed from
the cryogenic storage and at a lower temperature, special attention shall be paid to
raising the temperature of fibrinogen and dissolving solution to 30 °C ~ 37 °C, and
then dissolution is performed. Too low temperature tends to cause dissolution
difficulties and protein denaturation.
5 Model application
The type of dressing is different, the intended use is different, and the potential
adhesion is also quite different. Obviously, it is unreasonable to use the same
evaluation method (including test methods and test parameters) to evaluate the
potential adhesion of different dressings. Therefore, users of this Standard shall,
according to the material, intended use, and potential adhesion, etc. of the
dressing, design a suitable evaluation method, to obtain a reasonable
evaluation result.
1 - Briquetting block;
2 - Dressing sample A;
3 - Wound model (fibrin clot);
4 - Dressing sample B.
Note. If 0° without support [SEE Figure A.2a)] is used for the test, dressing sample A and
dressing sample B shall be in the form of opposite placement. This figure shows the
form of placement in the same direction.
Figure A.1 -- Illustration for the combination method of test dressings,
wound model, and briquetting block
TAKE the combination of the dressings and the wound model out from the
constant temperature-humidity chamber; PLACE in a drying oven to dry for 3 h
~ 4 h at (37±2)°C; TAKE out, and PLACE it to cool to room temperature.
The combination of the dressings and the wound model, according to one of
the methods shown in Figure A.2, is mounted on the clamps of the tensile tester,
so that the upper and lower clamps respectively hold two pieces of the test
dressing. The initial spacing of the two clamps is approximately 50 mm.
STRETCH at a rate of 100 mm/min, until one of the dressings is completely
peeled off from the wound model (fibrin clot). The way the sample is supported
during the test, that is, at diffe......
Related standard:   YY/T 1477.5-2020
Related PDF sample:   YY/T 1511-2017
   
 
Privacy   ···   Product Quality   ···   About Us   ···   Refund Policy   ···   Fair Trading   ···   Quick Response
Field Test Asia Limited | Taxed in Singapore: 201302277C | Copyright 2012-2020