Viscose filament yarn
| Valid |
GB/T 13758-1992 | English | 519 |
Add to Cart
|
4 days
|
Viscose filament yarn
| Obsolete |
Standards related to (historical): GB/T 13758-2008
Preview PDF (Powered by Google. Reload if blank, scroll for next page)
GB/T 13758-2008: PDF in English (GBT 13758-2008) GB/T 13758-2008
GB
NATIONAL STANDARD OF THE
PEOPLE’S REPUBLIC OF CHINA
ICS 59.060.20
W 52
Replacing GB/T 13758-1992
Viscose filament yarn
粘胶长丝
ISSUED ON: AUGUST 06, 2008
IMPLEMENTED ON: JUNE 01, 2009
Issued by: General Administration of Quality Supervision, Inspection and
Quarantine;
Standardization Administration of the People's Republic of
China.
Table of Contents
Foreword ... 3
1 Scope ... 4
2 Normative references ... 4
3 Terms and definitions ... 5
4 Product classification and marks ... 5
5 Technical requirements ... 6
6 Test methods ... 6
7 Inspection rules ... 8
8 Reinspection rules ... 9
9 Marks, packaging, transportation and storage ... 10
Annex A (normative) Inspection methods for appearance defects of viscose
filament yarn ... 12
Viscose filament yarn
1 Scope
This Standard specifies the requirements for product classification, technical
requirements, test methods, inspection rules and marks, packaging,
transportation, and storage of viscose filament yarn.
This Standard is applicable to the viscose filament yarn that is produced from
cotton pulp or wood pulp.
This Standard is applicable to the authentication and acceptance of the viscose
filament yarn of which the linear density is at 66.7dtex~333.3dtex. Dope colored
silk, the ones of which the linear density is below 66.7dtex and above 333.3dtex
can refer to this Standard as reference.
2 Normative references
The provisions in following documents become the provisions of this Standard
through reference in this Standard. For dated references, the subsequent
amendments (excluding corrigendum) or revisions do not apply to this Standard,
however, parties who reach an agreement based on this Standard are
encouraged to study if the latest versions of these documents are applicable.
For undated references, the latest edition of the referenced document applies.
GB/T 250, Textiles - Tests for colour fastness - Grey scale for assessing
change in colour
GB/T 1250, Rules for expression and judgement of limiting values
GB/T 3291.1, Textiles - Terms of textile material properties and test - Part 1:
Fibre and yarn
GB/T 3291.3, Textiles - Terms of textile material properties and test - Part 3:
General
GB/T 4146, Textiles - Man-made fibers
GB/T 6502, Sampling method for synthetic filament and textured yarns
GB/T 6503, Testing method for moisture regain of man-made fibers
GB/T 6504, Man-made fiber - Test method for oil content
GB/T 6529, Textiles - Standard atmospheres for conditioning and testing
GB/T 8170, Rules of rounding off for numerical values & expression and
judgement of limiting values
GB/T 14343, Testing method for linear density of man-made filament yarns
GB/T 14344, Testing method for tensile of man-made filament yarns
GB/T 14345, Testing method for twist of man-made filament
FZ/T 50014, Method for the determination of residual sulphur in viscose
fibers-direct iodimetry
FZ/T 50015, Test and assessment for dyeing uniformity of viscose filament
yarn
3 Terms and definitions
For the purposes of this document, the terms and definitions defined in GB/T
3291.1, GB/T 3291.3 and GB/T 4146 as well as the followings apply.
3.1 product lot
The serial production batch number with same raw materials, chemical
materials, auxiliary materials, process conditions and product specifications.
3.2 test lot
The test batch that is sampled periodically within a certain range so as to test
the stability of product quality during continuous production.
4 Product classification and marks
4.1 According to the different amount of matting agent or color paste added
during production, viscose filament yarn is divided into shiny yarn, matting yarn,
and colored yarn.
4.2 Product specifications are expressed by linear density (dtex) and number
of filaments (f). For example, for the yarn of which the linear density is 133.3dtex,
and the number of filaments is 30f, the specification is expressed as
133.3dtex/30f.
4.3 The product model is identified by the pulp, product specifications and
production process used in production. For example, 133.3dtex/30f cotton pulp
(bright) viscose filament yarn.
For the standard atmosphere for humidity control and test, according to GB/T
6529, the temperature is (20±2)°C and the relative humidity is (65±2)%. Pre-
conditioning temperature is less than 50°C and relative humidity is 10%~25%.
6.1.2 Sample preparation
6.1.2.1 Preparation of samples for measuring physical and mechanical
properties
6.1.2.1.1 Put each laboratory sample under standard atmospheric conditions to
adjust the humidity for 24h (the production plant allows humidity control for 1h
under normal conditions, but when the moisture regain of the sample exceeds
15%, the humidity should be adjusted for 24h). Then shake the sample.
6.1.2.1.2 Pull the laboratory sample off the surface silk. Use a length measuring
machine to shake 3 strands. Use the first 2 strands to determine the linear
density (fineness). Use the last 1 strand to determine the number of filaments,
dry fracture strength, wet fracture strength and elongation at break.
6.1.2.1.3 The 2 strands for measuring linear density and 1 strand for measuring
dry fracture strength and elongation shall be baked in an oven with a
temperature of 50°C to be lower than the public moisture regain (the production
plant can bake at 70°C for 30min). Then put them under standard atmospheric
conditions to absorb moisture for 2h~6h, so that the silk thread absorbs
moisture fully and reaches the moisture absorption balance.
6.1.2.1.4 The sample for measuring twist is obtained directly from the laboratory
sample.
6.1.2.2 Preparation of samples for determination of residual sulfur
Cut the sample into small pieces (about 2cm in length). Mix evenly. Put them
into a ground bottle to keep moisture.
6.2 Linear density and number of filaments
Strip the surface silk of each laboratory sample, in accordance with GB/T 14343.
6.3 Breaking strength and breaking elongation
Strip the surface silk of each laboratory sample, in accordance with GB/T 14344.
6.4 Twist
In accordance with GB/T 14345.
6.5 Residual sulfur
7.5.1 The grades for the physical and mechanical properties and dyeing and
chemical properties of a lot of products are conducted item by item according
to Table 1. The grades are respectively based on the rounding value
comparison method in GB/T 1250. The lowest grade is used as the highest
grade of this lot of products.
7.5.2 The appearance quality of each silk tube, silk skein, and silk cake in a lot
of products is graded based on Table A.1, Table A.2, Table A.3 in Annex A item
by item. The grades are respectively according to the rounding value
comparison method in GB/T 1250. The lowest grade is used as the grade of
each filament tube in this lot.
7.5.3 The grade of each silk tube (twist, cake) in a lot of products is determined
according to the lowest grade among the evaluation results of physical and
mechanical properties, dyeing properties and appearance defects.
7.5.4 The test data of each sample is based on one test and no retest is allowed.
If the tester finds an abnormality in the operation or the instrument, the tester
shall take a sample from the original laboratory sample and do it again after
taking measures. And use the redo data as the test result.
8 Reinspection rules
8.1 When the shipment arrives at the consignee, check whether the outer
packaging quality, number of pieces, and net quality of the package are
consistent with the manifest. If the quality problems are caused due to
transportation or storage process, it shall find out the reasons and the
responsibility shall be taken by the responsible party.
8.2 Within three months, if the product performance quality is found to be
inconsistent with the quality report, it can be submitted for re-inspection. If more
than one-third of this lot of products is used, no re-inspection is allowed.
8.3 For products within one year exited from the factory, if the quality of this lot
of products affects the quality of the post-processed products during use, and
causes serious losses, the supplier and the purchaser shall analyze the
reasons, clarify the responsibilities, and negotiate the treatment.
8.4 The inspection items during the reinspection are the same as those
specified in 7.2 inspection items.
8.5 The batching shall be conducted according to the original product lot during
reinspection.
8.6 The sampling method during the reinspection shall be carried out according
lot number, box number, official mass and actual weight, raw materials, storage
date and quality inspection employee number on it.
9.2 Packaging
9.2.1 The viscose filament yarn products are divided into tube, skein and cake.
The weight of the same lot of products, the weight of the tube, the skein and
the cake shall be consistent.
9.2.2 The packaging of the product shall be firm, safe, moisture-proof and easy
to transport to ensure that the product is not damaged.
9.2.3 Products of different lot numbers, varieties, grades and specifications
shall be packaged separately.
9.2.4 The moisture regain rate of the product during packaging shall be within
8%~15%. When exceeding, the humidity shall be adjusted to the specified
range before packaging.
9.3 Transportation
Handle with care during transportation. Prohibit damage to the outer packaging
and moisture.
9.4 Storage
This product shall be stacked in batches and stored in a dry and clean
warehouse. Must not stack in open air. Do not put it upside down and avoid
super high during storage to protect product quality from damage.
number of hairs with a length of less than 3mm (including loop hairs with a
vector length of less than 3mm) is greater than 20 (including the number of hairs
exceeding 3mm), it shall be reduced to a qualified product. A wounded thread
of which the single thread is not completely broken, is counted by the wool.
A.2.4.3 Knot: Refers to the connection after the thread breaks. During
inspection, the tubed yarn is counted directly from the small end, and the knot
shall be placed on the end of the small end of the yarn tube. The twisted yarn
is counted from the inside and outside two layers. If there is a broken head,
missed or wrong connection, it is regarded as out-of-class product.
A.2.4.4 Pollution: Refers to oily yarn, rusty yarn and stains that cannot be
washed off with water. During the inspection, when the total area contaminated
on the surface of the tube is not more than 6mm2, it shall be slightly oblivious.
When it does not exceed 8mm2, it shall be more obvious. When the number of
strands and the total length of the strands are less than 3 or the total length is
shorter than 20mm, it shall be slightly obvious. When the number of strands is
less than 7 or when the total length is shorter than 40mm, it shall be more
obvious. The cake-packed yarn is calculated according to the total pollution
area of the yarn cake. It shall be slightly obvious when it is less than 6mm2. It
shall be more obvious when it is less than 8mm2.
A.2.4.5 Curling: Refers to the regular bending and wrinkle points formed when
the thread is generated. When inspecting yarn skeins and yarn cakes, compare
with the standard sample respectively. The yarn cake with obvious curling shall
be out-of-class product.
A.2.4.6 Forming: Refers to the neatly winding condition of the yarn tube (cake)
layer. Do not press by hand during inspection.
When both ends of the paper tube of yarn tube shall protrude from the surface
of the yarn and the unevenness of the yarn layer is 7mm between the highest
and the lowest, it shall be the qualified product. When the difference between
the unevenness is less than or equal to 3mm, it shall be the first-class product.
When it is greater than 3mm, it shall be the qualified product. When the yarn
layer is flush with the tube, it shall be the qualified product. When the tube is
loose, it shall be reduced to the qualified product. When the inner and outer
layers of the yarn tube have two obvious elastic layers, it shall be quite good.
When there are three elastic layers, it shall be slightly bad. When it exceeds
three elastic layers, it shall be quite bad.
When the two ends of the cake-packed yarn are flush, it shall be good. When
there are unobvious size heads, it shall be slightly bad. When there are obvious
size heads, it shall be quite bad. When feathers appear on the surface of the
cake and tails appear on the inner layer, it shall be out-of-class product.